Inconel 600 vs Incoloy 800: Overview

Inconel 600 (UNS N06600) and Incoloy 800 (UNS N08800) are both nickel-based alloys widely used in high-temperature industrial service, but they are engineered around different balances. Inconel 600 is a nickel-chromium alloy with a very high nickel content of 72% minimum, making it ideal for general corrosion and high-temperature applications. Incoloy 800 is a nickel-iron-chromium alloy with a high iron content of about 40%, specifically designed for high-temperature strength, oxidation resistance and carburization resistance. In many cases Inconel 600 offers superior oxidation resistance, while Incoloy 800 performs better in creep and stress-rupture dominated high-temperature service.

Chemical Composition Compared

Inconel 600 contains nickel 72.0% min, chromium 14.0-17.0%, iron 6.0-10.0%, carbon 0.15% max, sulfur 0.015% max, silicon 0.50% max, manganese 1.00% max and copper 0.50% max.

Incoloy 800 contains nickel 30.0-35.0%, chromium 19.0-23.0%, iron 39.5% min, carbon 0.10% max, sulfur 0.015% max, silicon 1.00% max, manganese 1.50% max, copper 0.75% max, aluminum 0.15-0.60% and titanium 0.15-0.60%.

The high nickel content of 600 provides outstanding resistance to chloride stress corrosion cracking and caustic environments, while the aluminum and titanium additions in 800 support its high-temperature strength and oxidation resistance.

Mechanical Properties Compared

Annealed Inconel 600 typically shows a minimum tensile strength of about 655 MPa and yield strength of about 310 MPa, with a density of 8.47 g/cm3 and a melting point around 1413°C. Incoloy 800 typically shows a minimum tensile strength of about 520 MPa and yield strength of about 205 MPa, with a density of 7.94 g/cm3 and a melting point around 1385°C.

Compared with Alloy 600, Alloy 800 exhibits superior creep and stress-rupture properties at high temperature. Incoloy 800 can withstand temperatures up to about 1100°C, while the maximum applicable temperature for Alloy 600 is generally cited as about 1093°C.

Corrosion Resistance Compared

Both alloys exhibit excellent corrosion resistance, but with different strengths. Inconel 600 can withstand acidic environments and is widely used in the chemical industry. Incoloy 800 is renowned for its resistance to carburization and oxidation at high temperatures, which is why it is primarily used in hot furnace applications. When selecting between the two, the deciding factors are the corrosivity of the media and the dominant failure mechanism: chemical attack favors 600, while high-temperature carburization and creep favor 800.

Typical Applications

Inconel 600 is used to manufacture tempering furnaces, muffle furnaces, roller hearth furnaces and other furnace components, as well as heat treatment baskets and trays. In the aerospace industry it is used for engine and fuselage components that must withstand high temperatures, such as wiring harnesses, exhaust bushings and turbine seals. Incoloy 800 is preferred for hot furnace applications, heat treatment equipment and petrochemical heaters where carburization resistance and high-temperature creep strength are required.

Equivalents and Specification Notes

Inconel 600 corresponds to UNS N06600, W.Nr 2.4816, JIS NCF 600, AFNOR NC15FE11M, BS NA 13 and EN NiCr15Fe. Incoloy 800 corresponds to UNS N08800, W.Nr 1.4876, JIS NCF 800, AFNOR Z8NC32-21, BS NA 15 and EN X10NiCrAlTi32-20. Confirm the applicable ASTM or ASME specification for the product form, delivery condition and testing requirements with the supplier.

FAQ

Q: Which is stronger, Inconel 600 or Incoloy 800?

A: At room temperature Inconel 600 has higher minimum tensile strength, but at high temperatures Incoloy 800 exhibits superior creep and stress-rupture properties.

Q: Which alloy has a higher temperature limit?

A: Incoloy 800 can withstand temperatures up to about 1100°C, while the maximum applicable temperature for Alloy 600 is generally cited as about 1093°C.

Q: Is Incoloy 800 resistant to carburization?

A: Yes. Incoloy 800 is renowned for its resistance to carburization and oxidation at high temperatures, which makes it a primary choice for hot furnace applications.

Q: What is Inconel 600 used for?

A: Inconel 600 is used in tempering furnaces, muffle furnaces, roller hearth furnaces, heat treatment baskets and trays, and aerospace components such as exhaust bushings and turbine seals.

Q: What are the UNS numbers for these alloys?

A: Inconel 600 is UNS N06600 with W.Nr 2.4816, and Incoloy 800 is UNS N08800 with W.Nr 1.4876.

Q: Can Incoloy 800 be used in acidic chemical service?

A: Incoloy 800 has good general corrosion resistance, but for strongly acidic chemical service Inconel 600 is usually the better choice because of its higher nickel content.