What is the Inconel 625 Grade 1?
Inconel 625 Grade 1 refers to the annealed condition of the high-strength nickel alloy, characterized by specific mechanical properties (like lower yield strength in thicker sections) and a standard composition, making it a common choice for chemical processing, marine, and aerospace applications requiring excellent corrosion resistance, strength at high temperatures, and good weldability, often meeting specs like ASTM B446 and SAE AMS 5666.
What is Inconel 625 Grade 2?
Inconel 625 Grade 2 is a specific heat-treated form of the nickel-based superalloy Inconel 625, distinguished by its higher solution annealing temperature (around 1093°C/2000°F) compared to Grade 1, giving it superior strength, creep resistance, and excellent resistance to high-temperature corrosion and seawater, making it ideal for harsh aerospace, marine, and chemical processing environments.
What is the difference between 625 Grade 1 and Grade 2?
Inconel 625 Grade 2 is supplied in the Solution Annealed condition. The main difference between Grade 2 and Grade 1 is the annealing temperature. In the case of Grade 1, the minimum annealing temperature is 1600F (871degC), whereas for Grade 2 it is now 2000F (1093degC).
Inconel 625 Grade 1 vs Grade 2 – Mechanical Properties
| Property | Grade 1 | Grade 2 |
|---|---|---|
| Ultimate Tensile Strength (UTS) | 827 | 827 |
| Yield Strength (0.2% offset) | 414 | 414 |
| Elongation (in 50 mm) | 30 | 30 |
| Hardness (HRB) | 90–95 | 95–100 |
| Fatigue Strength | 310 | 310 |
| Impact Toughness (Charpy V-Notch) | ≥ 30 | ≥ 30 |
Inconel 625 Grade 1 vs Grade 2 – Thermal Properties
| Property | Grade 1 | Grade 2 | Unit |
|---|---|---|---|
| Melting Range | 1290–1350 | 1290–1350 | °C |
| Thermal Conductivity | 9.8 | 9.8 | W/m·K (25°C) |
| Specific Heat Capacity | 435 | 435 | J/kg·K |
| Coefficient of Thermal Expansion (20–100°C) | 12.8 | 12.8 | µm/m·°C |
| Maximum Service Temperature | 980 | 980 | °C |
What is the ASME specification for Inconel 625 alloy?
Inconel 625 alloy, numbered UNS N06625, has a nominal composition of 60Ni-22Cr-9Mo-3.5Cb.
Is Inconel 625 alloy magnetic?
Inconel 625 alloy is a non-magnetic, corrosion-resistant and oxidation-resistant nickel-chromium alloy. The high strength of Inconel 625 alloy comes from its strengthening combination of molybdenum and niobium added to the nickel-chromium matrix.
Heat Treatment:
Grade 1 steel is typically annealed at temperatures between 1600°F and 1800°F (approximately 871°C and 982°C) to provide good ductility and corrosion resistance while maintaining higher strength than Grade 2 steel.
Grade 2 steel is heat treated above 2000°F (about 1093°C) to enhance creep and stress rupture resistance while maintaining corrosion resistance.
Applications:
Grade 1 is typically used in marine, oil and gas, aerospace, and chemical processing applications.
Grade 2 is suitable for hydrogen production and hydrogen dissociation catalyst tubes where high temperature performance and corrosion resistance are critical.
The choice between Inconel 625 Grade 1 and Grade 2 primarily depends on your application environment and performance requirements.
Generally, Grade 1 is suitable for general chemical processing, seawater piping, and high-temperature heat exchangers due to its cost-effectiveness. However, for aerospace, nuclear industry, extreme corrosion, or high-pressure systems, Grade 2 is more appropriate because its strictly controlled microstructure and tolerances ensure long-term stable operation in demanding environments, reducing fatigue cracking and corrosion risks.
Based on long-term industrial data, Grade 2 exhibits a failure probability approximately 10–15% lower than Grade 1 in high-temperature, cyclic loading, and chloride environments, providing a higher safety factor for critical applications.
If you have project requirements for Alloy 625, we welcome your order. GNEE has a large inventory of popular products for you to choose from. It can be processed into various practical product forms, including plates, coils, tubes, bars, and wires. For detailed chemical composition information and free samples, please contact our factory immediately. We offer competitive prices and excellent service.