Jul 08, 2025 Leave a message

What Is The Difference Between Hastelloy C276 And B2 Alloy?

 

What Is The Difference Between Hastelloy C276 And B2 Alloy?

Hastelloy B2 and C276 are both nickel-based alloys known for their corrosion resistance, but they excel in different environments. Hastelloy B2 is primarily used in reducing environments, especially those containing hydrochloric acid, sulfuric acid and other non-oxidizing acids. Hastelloy C276, on the other hand, has a wider range of corrosion resistance, including both reducing and oxidizing environments.

What grades does Hastelloy C276 plate belong to?

The different grades include C22, C276, B-2 and Hastelloy X. Hastelloy C276 plate has 15% molybdenum and 14.5% chromium in its composition in addition to nickel. It is resistant to reducing, corrosive and oxidizing media.

What is the difference between Hastelloy C276 and Hastelloy B2

What is the difference between Hastelloy B2 and C22?

Hastelloy C22 has slightly higher strength and hardness than B2. This increased strength makes C22 ideal for applications that require higher mechanical loads. However, it is worth noting that the increase in strength may come at the expense of slightly reduced ductility.

What is the difference between 625 and C276?

Both Inconel 625 and Hastelloy C-276 are nickel-chromium-molybdenum based alloys. They both have excellent corrosion resistance and good strength. Comparing the two alloys, Inconel 625 has a higher chromium content, while Hastelloy C-276 has a higher molybdenum content.

Hastelloy C276 Vs B2 Alloy Chemical Composition

Comparison Table

The following table compares Hastelloy B2 and Hastelloy C276 based on their chemical composition and key performance characteristics:

Property Hastelloy B2 Hastelloy C276
Nickel (Ni) (%) 66.0 57.0
Molybdenum (Mo) (%) 28.0 16.0
Chromium (Cr) (%) 1.0 16.0
Iron (Fe) (%) 2.0 5.5
Cobalt (Co) (%) 1.0 2.5
Tungsten (W) (%) – 3.8
Manganese (Mn) (%) 1.0 0.5
Vanadium (V) (%) – 0.2
Silicon (Si) (%) 0.10 0.08
Carbon (C) (%) 0.02 0.01
Phosphorus (P) (%) 0.04 0.02
Sulfur (S) (%) 0.03 0.01
Corrosion Resistance Excellent in reducing acids, SCC resistance Excellent in wide range of corrosive environments, including chlorides
Mechanical Properties High strength and hardness High strength, toughness, and resistance to stress corrosion cracking
Weldability Easily weldable, no post-weld treatment required Weldable with precautions, post-weld treatment recommended
Applications Chemical processing, sulfuric acid production Chemical processing, oil and gas, pollution control
725

 

About Gnee Steel

Gnee Steel is a supplier of Hastelloy C276 And B2 Alloy, covering tubes: Seamless tubes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded tubes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy round bar sizes: diameter 3-800 mm;, Flat bar sizes: thickness 2-100 mm; Width: 10-500 mm, Hexagonal bar sizes: 2-100 mm;, Wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Hastelloy C276 And B2 Alloy, pipes, tubes, plates, strips, sheets, round bars, flat bars, forged billets, hexagons, wire rods and extruded profiles. You are welcome to contact us anytime to get a quote at ss@gneesteel.com

Send Inquiry

whatsapp

Phone

E-mail

Inquiry