What is N10276 material pipe?

N10276 (a nickel-chromium-molybdenum solid solution strengthened superalloy)
N10276/C276
UN number: N10276/2.4819
Common trade names: Hastelloy C276, SMC276

 

N10276 Alloy Tube Features
Alloy N10276 is a nickel-chromium-molybdenum solid solution strengthened superalloy with a nominal chemical composition of 57% nickel, 16% chromium and 16% molybdenum, with additions of iron, tungsten and cobalt. It is commonly referred to as Hastelloy® C276 and has a common designation of UNS N10276. C276 is often used in extremely corrosive environments that other alloys cannot withstand.

High Temperature Resistance
N10276 resists oxidation at temperatures up to 1900°F (1038°C).

Mechanical Properties
In the annealed condition, N10276 has a yield strength of 41ksi (345MPa). However, higher strengths can be achieved by the pilger process. N10276 maintains excellent toughness at cryogenic temperatures.

Heat Treatment
N10276 cannot be strengthened by heat treatment. C-276 is typically solution annealed at 2050°F (1121°C) followed by rapid cooling.

Machinability
N10276 can be hot worked in the temperature range of 1600°F to 2250°F (870°C to 1230°C). Annealing is recommended after hot working. Cold forming is possible, however, it has a high work hardening rate, so intermediate annealing may be required.

N10276 Hastelloy Alloy
Corrosion Resistance
N10276 is one of the most corrosion resistant alloys available. N10276 has excellent resistance to reducing and oxidizing acids, including sulfuric, hydrochloric, and acetic acids. It also performs well in seawater, chlorides, wet chlorine, oxidizing salts, and hypochlorites. The molybdenum and tungsten contents prevent various forms of localized corrosion, including pitting, crevice corrosion, and chloride stress corrosion cracking.
N10276 has excellent oxidation resistance at elevated temperatures up to 1900°F (1038°C). C-276 is not recommended for use in extreme oxidizing environments, such as concentrated hot nitric acid.