Dec 05, 2024 Leave a message

How much nickel is in Hastelloy C276?

‌Hastelloy C276 contains about 50-55% nickel‌‌.

 

Hastelloy C276 is a commonly used high-temperature alloy material, the main components of which include about 50-55% nickel (Ni), 16% chromium (Cr) and 16% molybdenum (Mo), in addition to a small amount of iron (Fe), tungsten (W) and other elements‌2. Its density is 8.89g/cm³, its melting point is between 1325-1370℃, and its tensile strength is 758MPa‌.

‌Hastelloy C276

Corrosion resistance: Hastelloy C276 exhibits excellent corrosion resistance in oxidizing and reducing media, including resistance to chlorides, sulfides, oxidants (such as nitric acid) and organic acids. It is particularly suitable for environments containing chlorides, such as wet chlorine, oxidizing chlorides, chloride salt solutions, sulfuric acid and oxidizing salts.

 

Hot working: The recommended hot working temperature range is 1100°C to 1175°C. In this temperature range, C276 can maintain good plasticity and processing properties. After hot working, it should usually be cooled to room temperature quickly to prevent recrystallization and grain growth.

 

Cold working: C276 can be cold worked by cold rolling, cold drawing, cold extrusion and other methods. Due to its high strength and hardness, cold working may be more difficult and requires more force and appropriate tools.

 

Welding performance: Hastelloy C276 has good welding performance, and commonly used welding methods include argon arc welding (TIG), stick arc welding (SMAW), etc. The same filler material as the base material should be used for welding, and the appropriate welding process should be adopted.

 

Application field: C276 is widely used in chemical process industry, petrochemical industry, marine facilities, paper industry, wastewater treatment and nuclear energy industry. It is particularly suitable for treating environments containing chloride ions or other chemicals.

 C276

Send Inquiry

whatsapp

Phone

E-mail

Inquiry