What are the differences between Inconel 600 sheet metal and 601 alloy steel sheet?

 

What are the differences between Inconel 600 sheet metal and 601 alloy steel sheet?

 

Gnee Steel is a well-known supplier of INCONEL 600 and INCONEL 601 alloy plates. These plates are widely used in high-temperature environments, exhibiting excellent strength and heat resistance. They maintain superior mechanical properties and durability even after long-term use under various conditions. Furthermore, they possess good formability and weldability, facilitating processing and application. With their excellent workability, low maintenance costs, and affordable price, these alloy plates offer significant advantages.

What are the differences between Inconel 600 sheet metal and 601 alloy steel sheet
Nickel Alloy 600 and Inconel 600

Are Nickel Alloy 600 and Inconel 600 the same alloy?

 

Nickel Alloy 600, also sold under the brand name Inconel 600, is a unique nickel-chromium alloy known for its oxidation resistance at high temperatures. It has a wide range of applications, suitable for high-temperature applications from low temperatures up to 2000°F (1093°C).

INCONEL 600 steel plate is suitable for various corrosive media and exhibits excellent resistance to acids, alkalis, and chlorides. Therefore, it effectively prevents pitting, cracking, and other corrosive effects caused by chlorides. This steel plate has good corrosion resistance in atmospheric environments and its surface is finished using various processes such as hot rolling, cold rolling, polishing, and satin coating, making it resistant to rust. Its excellent hardness reduces stress effects under high loads. Depending on the application, INCONEL 600 steel plate is available in various hardness grades, including soft, hard, semi-hard, quarter-hard, and spring-hard.


INCONEL 601 steel plate is an aluminum-rich steel plate with higher strength and toughness. It is an excellent water-based material, effectively preventing corrosion from high-purity water and acidic corrosion. It also effectively prevents oxidation and carburization, and has a significant inhibitory effect on chloride-induced corrosion. Furthermore, its excellent crack resistance and fracture strength effectively prevent stress cracking under extreme temperature conditions.

 

INCONEL 6OO/6OI Sheet Material Specifications

Standard: ASTM B168/ASME SB168
Dimensions: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm

Forms: Roll, Foil, Sheet, Flat, Strip, Flat, Blank (Round), Ring (Flange), etc.

Hardness: Soft, Hard, Semi-hard, Quarter-hard, Spring Hard, etc.

Thickness: 0.1 mm to 12 mm

Length: 500 mm to 12000 mm

Width: 100 mm to 3000 mm

 

Inconel 600 / 601 Plate Equivalent Grades

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 600 2.4816 N06600 NCF 600 NA 13 МНЖМц 28-2,5-1,5 NC15FE11M NiCr15Fe
Inconel 601 2.4851 N06601 NCF 601 NA 49 XH60BT NC23FeA NiCr23Fe

 

Inconel 600 / 601 Plate Types

Plates Suppliers, Stockist In India

Inconel 600 / 601 Plate

ASME SB168 601 Alloy Plate

ASTM B168 Inconel 600 Plate Exporter

Inconel Alloy 600 Plate Stockholder

601 Nickel Alloy Plate Distributor

Nickel Alloy 2.4816 Plate Trader

Inconel UNS N06600 Plate Supplier

Cold Rolled Plate

Inconel 600 / 601 Cold Rolled Plate

Inconel ASTM B168 600 Cold Rolled Sheet Exporter

Inconel 601 Cold Rolled Sheet Supplier

ASME SB168 600 Alloy Cold Rolled Sheet

Inconel Alloy 601 Cold Rolled Sheet Stockholder

Inconel 2.4851 Cold Rolled Sheet Trader

Cold Rolled Nickel Alloy UNS N06601 Sheet Distributor

Hot Rolled Plate

Inconel 600 / 601 Hot Rolled Plate

Inconel 601 Alloy Hot-Rolled Sheet Stockholder

Inconel UNS N06601 Hot-Rolled Sheet Supplier

Inconel 2.4816 Cold-Rolled Sheet Trader

Inconel ASTM B168 600 Hot-Rolled Sheet Exporter

Hot-Rolled Nickel Alloy 601 Sheet Distributor

ASME SB168 600 Alloy Hot-Rolled Sheet

Inconel 600 / 601 Plate Dimension

Dimension (mm) KG P/M2
0.5 X 1000 X 2000 4.5
0.7 X 1219 X 3048 6.3
0.9 X 1219 X 3048 8.1
1.2 X 1219 X 3048 10.8
1.6 X 1200 X 3048 14.4
2.0 X 1219 X 3048 18.0
3 X 1200 X 3000 27.0
3.18 X VARIOUS ANN 28.6

 

Chemical Composition of Inconel 600 / 601 Plate

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00
Inconel 601 0.10 max 1.0 max 0.5 max 0.015 max 1.0 max Balance 58.0 – 63.0 21.0 – 25.0

 

Mechanical Composition of Inconel 600 / 601 Plate

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %
Inconel 601 8.1 g/cm3 1411 °C (2571 °F) Psi – 80,000 , MPa – 550 Psi – 30,000 , MPa – 205 30 %

 

Inconel 600/601 alloy sheet applications

 

Oil and Gas Industry

Pulp and Paper Industry

Power Plants

Energy Industry

Modern Construction

Fluid Piping

Dairy and Food Processing

Heat Exchangers

Textile Machinery

Wastewater Treatment Projects

Synthetic Fibers

Exhaust Gases and Emissions

Construction Industry

Automotive Industry

Material Transportation

Inconel 600/601 alloy sheet applications

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 

Contact now

Gnee Steel also supplies custom Inconel 600 products in various sizes and specifications. Please send us your drawings for a quote!

 

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 alloy, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness: 0.1 to 100 mm; width: 10-2500 mm); strips; alloy round bars (diameter: 3-800 mm); flat bars (thickness: 2-100 mm; width: 10-500 mm); hexagonal bars (size: 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with Inconel 600 alloy products that meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.