Weight chart for Alloy 601 pipe fittings

 

601 alloy (UNS NO6601) pipe fittings are high-nickel corrosion-resistant components with a density of 8.11 g/cm³. They are typically supplied in butt-weld form (elbows, tees, reducers) in sizes ranging from 1/2 inch to 48 inches, conforming to ASTM B366 and ASME B16.9 standards, with wall thicknesses covering Schedule 5 to XXS grades.

 

Buttweld Pipe Fittings Weight Chart

DN Schedule 10S Schedule 40S Schedule 80S
Con reducer Ecc reducer Reducing tee Con reducer Ecc reducer Reducing tee Con reducer Ecc reducer Reducing tee
40x.25 0.19 0.19 0.60 0.26 0.26 0.76 0.34 0.34 0.90
50x25 0.28 0.28 0.73 0.40 0.40 1.10 0.54 0.54 1.37
50x40 0.31 0.31 0.76 0.45 0.45 1.15 0.59 0.59 1.43
80x.50 0.55 0.55 1.56 1.00 1.00 2.91 1.79 1.79 3.91
100x50 0.78 0.78 2.94 1.50 1.50 4.48 1.95 1.95 6.55
100x80 0.87 0.87 3.04 1.74 1.74 4.64 2.33 2.33 6.79
150x80 1.82 1.82 6.86 3.95 3.95 9.68 5.51 5.51 11.57
150x100 1.96 1.96 7.10 4.07 4.07 11.94 5.96 5.96 11.97
200x100 3.01 3.01 13.46 6.55 6.55 17.98 9.23 9.23 24.18
200x150 3.19 3.19 14.08 6.74 6.74 18.82 10.12 10.12 25.31

 

Welded Butt Welding Fittings – ASTM A403M & ASME B16.9

Product range and theoretical weights (kg)
DN Schedule 10S Schedule 40S
900
Elbow
450
Elbow
Equal tee Stub end type B End cap 900
Elbow
450
Elbow
Equal tee Stub end type B End cap
15 0.06 0.03 0.09 0.07 0.03 0.08 0.04 0.10 0.08 0.04
20 0.07 0.03 0.13 0.09 0.05 0.08 0.04 0.17 0.11 0.07
25 0.14 0.08 0.28 0.16 0.08 0.15 0.11 0.29 0.17 0.10
32 0.23 0.11 0.49 0.22 0.10 0.26 0.17 0.59 0.25 0.18
40 0.30 0.17 0.68 0.25 0.11 0.40 0.23 0.86 0.31 0.20
50 0.50 0.25 0.85 0.43 0.13 0.70 0.40 1.28 0.61 0.23
65 0.85 0.48 1.41 0.57 0.19 1.40 0.77 2.19 0.80 0.27
80 1.25 0.63 1.77 0.72 0.25 2.20 1.08 3.31 1.13 0.42
100 2.10 1.08 3.46 1.09 0.68 4.47 1.47 5.27 1.87 1.14
125 3.65 1.82 5.44 1.47 1.11 6.80 2.84 9.63 2.79 2.13
150 5.45 2.72 8.03 2.15 1.42 10.89 5.44 10.99 3.57 3.23
200 10.20 5.33 15.65 3.22 2.38 21.54 10.77 20.91 6.07 5.19
250 18.15 9.75 26.76 5.13 4.45 38.56 19.27 35.38 10.07 9.00
300 25.80 13.62 39.46 8.16 7.50 59.42 29.71 62.14 14.29 15.00
350 36.29 18.37 48.53 10.88 8.17 79.38 35.15 79.31 17.14 16.00
400 47.63 23.81 58.97 12.70 10.67 99.79 45.81 99.79 20.41 21.00
450 59.87 29.94 79.65 17.23 13.00 129.73 59.40 129.73 27.21 26.00
500 99.80 49.90 103.42 21.77 17.00 162.38 74.84 162.39 29.94 34.00
600 140.61 70.31 155.58 27.21 26.00 225.89 105.23 225.90 38.55 52.00

 

Welded Butt Welding Fittings – ASTM A403M & ASME B16.9

Product range and theoretical weights (kg)
DN Schedule 10S Schedule 40S
Con reducer Ecc reducer Reducing tee Con reducer Ecc reducer Reducing tee
20x15 0.10 0.10 0.11 0.14 0.14 0.15
25x15 0.12 0.12 0.25 0.15 0.15 0.26
25x20 0.13 0.13 0.25 0.16 0.16 0.27
32x20 0.18 0.18 0.44 0.22 0.22 0.52
32x25 0.18 0.18 0.45 0.22 0.22 0.53
40x20 0.18 0.18 0.58 0.24 0.24 0.74
40x25 0.19 0.19 0.60 0.26 0.26 0.76
40x32 0.21 0.24 0.61 0.28 0.28 0.77
50x25 0.28 0.28 0.73 0.40 0.40 1.10
50x32 0.30 0.30 0.74 0.44 0.44 1.13
50x40 0.31 0.31 0.76 0.45 0.45 1.15
65x40 0.44 0.44 1.24 0.76 0.76 1.94
65x50 0.47 0.47 1.25 0.80 0.80 1.98
80x40 0.51 0.51 1.52 0.94 0.94 2.85
80x50 0.55 0.55 1.56 1.00 1.00 2.91
80x65 0.59 0.59 1.59 1.08 1.08 2.98
100x40 0.68 0.68 2.90 1.36 1.36 4.53
100x50 0.78 0.78 2.94 1.57 1.57 4.48
100x65 0.83 0.83 2.97 1.66 1.66 4.54
100x80 0.87 0.87 3.04 1.74 1.74 4.64
125x100 1.49 1.49 5.49 2.98 2.98 8.47
150x80 1.82 1.82 6.86 3.98 3.98 11.94
150x100 1.96 1.96 7.10 4.07 4.07 9.68
150x125 2.00 2.00 7.27 4.07 4.07 9.99
200x100 3.01 3.01 13.46 6.55 6.55 17.98
200x150 3.19 3.19 14.08 6.94 6.94 18.82
250x100 4.73 4.73 22.75 10.52 10.52 30.07
250x150 5.00 5.00 23.55 11.12 11.12 31.13
250x200 5.20 5.20 24.08 11.56 11.56 31.84
300x200 7.67 7.67 34.73 15.98 15.98 54.43
300x250 7.98 7.98 35.52 16.63 16.63 55.79
350x300 15.29 15.29 43.96 30.58 30.58 71.21
400x200 16.70 16.70 49.90 33.40 33.40 84.82
400x250 17.22 17.22 50.80 35.43 35.43 85.73
400x300 18.35 18.35 51.71 36.70 36.70 87.54