Detailed explanation of Inconel 601 rod size chart

601 alloy round bar size chart, China Inconel 601 round bar size chart, 601 steel bar size chart (millimeters), 601 steel bar weight and size chart (kilograms).

 

Inconel 601 rod size chart

ize in mm Average Weight
KG/MTR KG/FT
10 0.62 0.18
12 0.90 0.30
14 1.20 0.40
16 1.60 0.50
18 2.00 0.60
20 2.50 0.80
22 3.00 0.90
24 3.56 1.08
25 3.90 1.20
28 4.80 1.50
30 5.55 1.69
32 6.30 1.90
34 7.14 2.18
36 8.00 2.44
40 9.90 3.00
45 12.49 3.81
50 15.40 4.70
56 19.34 5.89
60 22.20 6.80
63 24.47 7.46
63.5 24.86 7.58
65 26.05 7.94
70 30.20 9.20
73 32.86 10.00
75 34.72 10.58
78 37.51 11.43
80 39.50 12.00
83 42.47 12.95
85 44.55 13.58
90 50.00 15.20
92 52.19 15.91
93 53.39 16.27
95 55.65 16.95
100 61.66 18.79
105 67.98 20.72
110 74.60 22.74
115 81.64 24.88
125 96.34 29.36