What UNS N06686 Is
UNS N06686 is a single-phase austenitic nickel-chromium-molybdenum-tungsten alloy developed for severe corrosion service in both reducing and oxidising media. It combines the molybdenum level of the classic Ni-Cr-Mo alloys with a deliberate tungsten addition, and holds carbon, silicon and iron at low levels so that weld heat-affected zones retain their corrosion resistance without a post-weld solution anneal on thin sections. The alloy is not a precipitation-hardening grade; it obtains its strength from solid-solution alloying and is supplied in the annealed condition.
Its commercial significance is that it covers three duties that usually require different alloys: chloride-bearing solutions where pitting and crevice attack are the failure mode, reducing acids where nickel and molybdenum carry the protection, and oxidising media where chromium and molybdenum work together. A material selector who would otherwise need two grades for two parts of the same plant can often use one.
Chemical Composition and Metallurgy
| Element | Limits per ASTM B575 (UNS N06686) | Function |
|---|---|---|
| Nickel | Balance | Stabilises the austenitic matrix; provides resistance in reducing media and against chloride stress corrosion cracking |
| Chromium | 19.0-23.0 % | Passive film formation in oxidising conditions |
| Molybdenum | 15.0-17.0 % | Pitting and crevice corrosion resistance; resistance to reducing acids |
| Tungsten | 3.0-4.4 % | Further improves localised corrosion resistance |
| Iron | 5.0 % max | Residual; kept low to preserve corrosion resistance |
| Carbon | 0.010 % max | Kept very low to prevent grain-boundary carbide precipitation |
| Silicon | 0.08 % max | Kept low to limit intermetallic phase formation |
| Manganese | 0.75 % max | Deoxidation residual |
| Copper | 0.50 % max | Residual |
| Titanium | 0.02 % max | Controlled to avoid undesirable phases |
The very low carbon and silicon limits are what make the alloy tolerant of welding in the as-welded condition. Intermetallic phases such as mu phase form in this type of chemistry when carbon and silicon are high, and their appearance at grain boundaries is what destroys ductility and corrosion resistance after exposure to elevated temperature.
Corrosion Performance
The alloy's pitting resistance equivalent number, calculated as Cr + 3.3 Mo + 16 N from the specification mid-range, falls near the top of the wrought nickel-alloy range because of the combined molybdenum and tungsten content. Reported behaviour, taken from published corrosion data for the grade, is as follows:
Oxidising chloride media. Very high resistance to pitting and crevice corrosion, including in acidic chloride solutions where 316L and 6 % molybdenum stainless steels fail by localised attack.
Reducing acids. Good resistance in sulphuric and phosphoric acid over wide concentration ranges, and in mixed acid environments.
Oxidising salts and hypochlorite. Useful resistance where chloride and oxidising species occur together, a combination that defeats many nickel alloys.
Stress corrosion cracking. High resistance in chloride-bearing environments and in high-temperature water; the high nickel content and the austenitic matrix are both favourable.
Intergranular attack. Resistant in the as-welded condition because carbon is limited to 0.010 %.
Corrosion testing for this class of material is normally specified to ASTM G48, which uses ferric chloride solution to rank pitting and crevice resistance, and to ASTM G28 for intergranular corrosion. Test temperature and finishing condition must be stated, because both change the result substantially.
Physical and Mechanical Data
| Property | Typical value |
|---|---|
| Density | 8.73 g/cm³ |
| Melting range | 1338-1380 °C |
| Elastic modulus at room temperature | Approx. 207 GPa |
| Electrical resistivity, 20-700 °C | Approx. 1.24-1.28 microhm-metre |
| Mean linear expansion, 100-600 °C | Approx. 12.0-13.2 micrometre per metre per kelvin |
| Specific heat, 20-700 °C | Approx. 377-519 J/kg·K |
| Crystallographic structure | Face-centred cubic austenite |
These figures are published reference values for the annealed wrought product and are used for thermal stress and heat transfer calculations. They are not acceptance values; acceptance values are the tensile properties stated in the applicable product specification.
Product Forms and Specifications
| Form | Specification |
|---|---|
| Rod and bar | ASTM B574 |
| Plate, sheet and strip | ASTM B575 |
| Seamless tube | ASTM B622 |
| Welded pipe | ASTM B619 |
| Welded tube | ASTM B626 |
| Forgings and fittings | ASTM B564 and ASTM B366 |
Fabrication Notes
Machining is done with carbide tooling at lower surface speed than for stainless steel, and the alloy work-hardens quickly, so depth of cut should stay generous while feed is steady. Forming in the annealed condition is practical for sheet and plate; heavy cold forming raises strength and reduces ductility and may require an intermediate anneal. Welding uses matching nickel-alloy filler and practices suitable for Ni-Cr-Mo material: clean joint faces, no preheat, controlled interpass temperature, and complete removal of heat tint. Because carbon is limited to 0.010 %, the as-welded corrosion resistance is good, but in thick sections or in the most aggressive duties a post-weld solution anneal and water quench is used to restore the best properties.
Frequently Asked Questions
Q: Which product-form specification applies to N06686 plate?
A: ASTM B575 covers plate, sheet and strip of UNS N06686 and the related low-carbon Ni-Cr-Mo alloys. Bar and rod are covered by ASTM B574, and seamless tube by ASTM B622.
Q: Can N06686 be used above 600 °C?
A: It is primarily a corrosion alloy. Continuous exposure at elevated temperature can form intermetallic phases in this type of chemistry, so high-temperature structural duty is normally assigned to an oxidation- and creep-resistant grade instead.
Q: Why are carbon and silicon limits so tight?
A: Carbon and silicon both promote the formation of intermetallic phases at grain boundaries during welding and elevated-temperature exposure. Holding carbon at 0.010 % max and silicon at 0.08 % max keeps those phases out and preserves ductility and corrosion resistance.
Q: Is a post-weld heat treatment required after welding?
A: Not for thin sections in most services. Where the section is thick, or where the service is highly aggressive, a solution anneal followed by rapid cooling restores the optimum structure. The decision belongs in the welding procedure specification.
Q: How should the alloy be selected against a 6 % molybdenum super-austenitic stainless steel?
A: The nickel alloy is chosen when the chloride concentration, acidity or temperature exceed what the stainless steel will survive, when crevices cannot be eliminated by design, or when mixed oxidising and reducing conditions occur. A ferric chloride corrosion test at service temperature on both candidate materials is the most reliable way to make the decision.
Q: What finished-product documentation is normally required?
A: A certificate of compliance with the product specification, chemical analysis, tensile test results, heat treatment condition, and corrosion test results where specified. Traceability from heat number to the finished component is expected for pressure and chemical service.