Nondestructive Testing of Nickel-Based Alloys 200

Nondestructive Testing of Nickel-Based Alloys 200

Alloys 200 Mechanical Properties

Tensile Strength 380 MPa (55,000 psi) minimum
Yield Strength 105 MPa (15,000 psi) minimum
Elongation 30% minimum (in 2-inch gauge length)
Hardness HRB 45-70 (Typical)

Nickel Alloys 200 Physical Properties

Density 8.89 g/cm³
Melting Range 1446°C (2635°F)
Thermal Conductivity 70.2 W/m·K (at 20°C)
Electrical Resistivity 9.6 μΩ·m (at 20°C)
Modulus of Elasticity 204 GPa (29.6 x 10^6 psi)

Nickel 200 Chemical Composition (% By Weight)

Element Min Max
Ni 99 -
Fe - 0.4
Mn - 0.35
C - 0.15
Cu - 0.25
Si - 0.35
S - 0.01