Dec 25, 2023 Leave a message

MonelK500 is commonly known as Monel K500

MonelK500 is commonly known as Monel K500

 

1. Introduction to Monel K500:

Monel K500 actually has the same corrosion resistance as Monel400, but has higher mechanical strength and hardness than 400. It also has better hot corrosion resistance and long-term organizational stability. However, the plasticity is slightly lower than that of Monel K500. Compared with Monel400, this alloy contains a mass fraction of 2.3%~3.15% aluminum AL and 0.3%~1.00% titanium Ti. The amount added is different in different places.

2. Monel K500 applications and features:

Monel K500 alloy has good low-temperature plasticity and toughness, so you won't find any difficulty in cold working. However, in terms of hot working, the forming temperature is generally between 871 and 1149 degrees, and the large deformation is between 1038 and 1149 degrees. However, we recommend that the appropriate temperature should be between 1093 degrees, the alloy solution annealing temperature is 793~971, and good comprehensive properties can be obtained.

MonelK500 is commonly known as Monel K500

MonelK500 is commonly known as Monel K500

The temperature of hot-processed products should be 982 degrees, and the temperature of cold-processed products should be 1038 degrees, but the heating time should be shortened as much as possible. Most uses of Monel K500 alloy are the same as 400, but if there are applications other than 400, this alloy can be used. Monel K500 alloy is mainly used in pump shafts, impellers, conveyor scrapers, oil drill rings, strong components, valve parts and papermaking equipment. Squeegee blades, etc.

3. Monel K500 material specifications:

Hot-rolled rods 15~100mm, forged rods: 100mm~350mm, cold-rolled thin plates 0.05mm-4.0mm, hot-rolled plates: 4mm~14mm, strips 2mm-10mm, forgings of various sizes, etc.

4. Monel K500 processing and welding performance

Monel K500 alloy has good low-temperature plasticity and toughness, so you won't find any difficulty in cold working. However, in terms of hot working, the forming temperature is generally between 871 and 1149 degrees, and the large deformation is between 1038 and 1149 degrees. However, we recommend that the appropriate temperature should be between 1093 degrees, the alloy solution annealing temperature is 793~971, and good comprehensive properties can be obtained. The temperature of hot-processed products should be 982 degrees, and the temperature of cold-processed products should be 1038 degrees, but the heating time should be shortened as much as possible. Different welding methods of Monel K500 alloy require different welding wires. Generally, Monel64 and 134 welding wires are selected.

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry