Dec 25, 2023 Leave a message

Monel400 material composition Monel400 physical and mechanical properties

Monel400 material composition Monel400 physical and mechanical properties

 

Monel 400 alloy (UNS N04400 or MCu-28-1.5-1.8 or Ni68Cu28Fe) is a kind of alloy that can be used in seawater, chemical solvents, ammonia sulfur chloride, hydrogen chloride, various acidic media such as sulfuric acid, hydrofluoric acid, hydrochloric acid, phosphoric acid, organic acids , a nickel-based alloy material with good corrosion resistance in alkaline media, salt and molten salt.

Chinese name

Monel 400 alloy

heat conduction

21.8 W/m-K

melting point

1300 - 1350°C

Monel400 material composition Monel400 physical and mechanical properties

Monel400 material composition Monel400 physical and mechanical properties

Magnetism

200H(At 70F)

Introduction

Monel 400 alloy also has good mechanical properties, a wide range of use temperatures from low to high temperatures, good welding properties and medium and high strength.

application

Monel 400 is mainly used in chemical and petrochemical industries, as well as marine development and other fields. It can be used to manufacture various heat exchange equipment, boiler feed water heaters, petroleum and chemical pipelines, containers, towers, tanks, valves, pumps, reactors, shafts, etc.

Implementation standards

ASTM B 164 (rods, wires), ASTM B 564 (forgings), ASTM B 127 (plates, strips), ASTM B 165 (seamless pipes).

processing

The alloy can be machined using the same methods as traditional iron-based materials. Use water coolant when adding high speed machines. The material shrinks during processing, so attention should be paid to the processing shrinkage allowance to ensure dimensional accuracy.

welding

Monel 400 has good welding performance and can use TIG and MIG methods. It can use Monel body or EniCu-7 wire and electrode; or manual arc welding and submerged arc welding; it can be welded with carbon steel and low alloy steel.

 