Inconel718 alloy is a precipitation-hardened nickel-chromium-iron alloy containing niobium and molybdenum. It has high strength, good toughness and corrosion resistance in high and low temperature environments below 650℃.
Incone l 718 similar grades:
N07718, GH4169, GH169 (China), NC19FeNb (France), W.Nr.2.4668, NiCr19Fe19Nb5 (Germany)
The supply state can be solution treated or precipitation hardened. During hot working, the material should be heated to the upper limit of the processing temperature. In order to ensure the plasticity during processing, the final processing temperature when the deformation reaches 20% should not be lower than 960℃.
The oxide near the weld of Inconel718 workpiece is more difficult to remove than that of stainless steel. It needs to be polished with fine sand belt. Before pickling in a mixed acid of nitric acid and hydrofluoric acid, the oxide should also be removed with sandpaper or salt bath pretreatment should be performed.
Main specifications of Inconel718 supplied by GNEE:
Inconel 718 seamless pipe, Inconel 718 steel plate, Inconel 718 round steel, Inconel 718 forgings, Inconel 718 flanges, Inconel 718 welded pipes, Inconel 718 steel strips, Inconel 718 straight bars, Inconel 718 wires, Inconel 718 flat steel, Inconel 718 hexagonal bars, Inconel 718 elbows, Inconel 718 tees, Inconel 718 machined parts, Inconel 718 bolts and nuts, Inconel 718 fasteners.