Nickel 718, also known as Inconel 718, is a precipitation-hardened nickel-based high-temperature alloy with high strength, corrosion resistance and good welding properties. This alloy exhibits excellent comprehensive properties in the temperature range of -253℃ to 700℃, especially below 650℃, its yield strength ranks first among deformable high-temperature alloys.
Nickel 718 physical properties:
Density: about 8.19 g/cm³
Melting point: 1260-1336°C
Specific heat capacity: 435 J/(kg·K)
Thermal conductivity: 11.4 W/(m·K) (at 20°C)
Inconel 718 mechanical properties:
Tensile strength (σb): 965 MPa
Yield strength (σ0.2): 550 MPa
Elongation (δ): 12-20%
Sectional reduction (ψ): 30-40%
Hardness: ≤331 HB
Inconel Alloy 718 heat treatment:
The heat treatment of Inconel 718 alloy usually includes solution treatment and aging treatment to obtain the best mechanical properties. Typical heat treatment steps include:
Solution treatment: keep at 980-1010°C for 1 hour, followed by rapid cooling.
Aging treatment: The first step is to keep it at 720°C for 8 hours, then cool it down to 620°C at a rate of 50°C/hour; the second step is to keep it at 620°C for 8 hours, then air cool it.

Due to its excellent high-temperature performance, Inconel 718 alloy is widely used in the following fields:
Aerospace: used to manufacture key components such as aircraft engines, turbine blades, combustion chambers and nozzles.
Energy: used for containers, pipes and equipment in nuclear power plants, as well as wind turbines and solar power generation equipment.
Petrochemical: used to manufacture high-temperature and high-pressure valves, pipes and heat exchangers and other equipment.