Is Alloy 800 (UNS N08800) Stainless Steel? Composition and Properties

Is Alloy 800 a Stainless Steel or a Nickel Alloy?

Alloy 800 (UNS N08800) is a nickel-iron-chromium alloy that sits at the boundary between the austenitic stainless steel family and the nickel-base high-temperature alloy family. Its chromium content of 19.0-23.0 % is high enough to form the protective chromium oxide film that defines stainless steel. Its nickel content of 30.0-35.0 %, by contrast, is far above the 8-12 % typical of ordinary 300-series grades, which is why standards bodies and metallurgists normally classify it as a nickel-iron-chromium superalloy rather than a conventional stainless steel. In commercial practice both descriptions are used, and neither is unreasonable: the alloy is fully austenitic, it is iron-bearing, and it is selected for exactly the combination of corrosion resistance, strength and high-temperature stability that stainless steel users are looking for.

What Separates Alloy 800 from Standard Stainless Steel

Three differences matter in service. The first is structural stability: the high nickel content holds the austenitic structure in place, so the alloy remains ductile and non-magnetic even after long exposure at temperature. The second is the deliberate addition of titanium and aluminium, which allows the alloy to resist sensitisation and to form a fine dispersion of carbides and nitrides during service, giving it unusually good resistance to oxidation and carburisation above 500 °C. The third is corrosion behaviour: the chromium-nickel balance delivers excellent resistance to chloride stress corrosion cracking, to dilute sodium hydroxide solutions and to high-temperature, high-pressure water, which is why the grade is specified for stress-corrosion-critical equipment such as heat exchangers and nuclear steam generator tubing.

Chemical Composition of Alloy 800 (UNS N08800)

The grade is covered by ASTM B409 for hot-rolled plate, ASTM B514 for cold-rolled plate and ASTM B515 for cold-rolled strip. Typical composition limits are:

Element Content (wt %)
Nickel (Ni) 30.0-35.0
Chromium (Cr) 19.0-23.0
Iron (Fe) 39.5 minimum, balance
Carbon (C) 0.10 maximum
Manganese (Mn) 1.50 maximum
Silicon (Si) 1.00 maximum
Copper (Cu) 0.75 maximum
Aluminium (Al) 0.15-0.60
Titanium (Ti) 0.15-0.60
Sulfur (S) 0.015 maximum

Mechanical, Physical and Corrosion Properties

In the solution-annealed condition the alloy combines moderate room-temperature strength with high ductility, and it keeps a useful fraction of that strength as the temperature rises. The figures below are typical for solution-annealed product; actual values depend on product form, size and heat treatment.

Temperature Short-time tensile strength
Room temperature about 450 MPa
100 °C 425 MPa
300 °C 390 MPa
500 °C 360 MPa
600 °C 300 MPa

Density: 7.94 g/cm³

Melting range: 1350-1400 °C

Thermal conductivity at 200 °C: about 11-12 W/(m·K)

Modulus of elasticity: about 196 GPa

Magnetism: non-magnetic, because the structure is fully austenitic

Typical 0.2 % yield strength: about 170 MPa, with elongation of about 30 % in the annealed condition

Corrosion performance is the main reason the grade exists. Its resistance is better than that of general-purpose austenitic stainless steels and better than the 600-series nickel-chromium-iron alloy in several stress-corrosion environments, particularly in chloride-bearing and caustic media and in high-purity water.

Processing, Heat Treatment and Welding

Hot working is carried out in the range 1200 °C down to 950 °C, followed by water quenching or rapid air cooling, and a solution treatment should always follow hot working so that the best combination of properties and creep resistance is restored. Cold working hardens the material faster than it hardens austenitic stainless steel, so heavier equipment is needed, the starting stock should be in the solution-treated condition, and an intermediate anneal is advisable when the reduction is large. A secondary solution treatment is required once the cold reduction exceeds 10 %.

The alloy is welded with all of the conventional processes, including gas tungsten arc, plasma arc, gas metal arc and submerged arc welding; pulsed arc welding is usually the first choice for thin sections. Filler selection normally matches the base metal composition, and shielding gas mixtures based on argon with helium, hydrogen and carbon dioxide additions are widely used.

Frequently Asked Questions

Q: Is Alloy 800 stainless steel?
It is an austenitic, iron-bearing, chromium-bearing alloy, so it behaves in many ways like stainless steel, but its 30-35 % nickel content places it in the nickel-iron-chromium family used for high-temperature service.

Q: What is the composition of Alloy 800?
Roughly 30-35 % nickel, 19-23 % chromium and iron as the balance, with small controlled additions of titanium and aluminium; carbon is held to 0.10 % maximum.

Q: Is Alloy 800 magnetic?
No. Its fully austenitic structure is non-magnetic, and it stays non-magnetic after high-temperature service exposure.

Q: How does Alloy 800 differ from 304 stainless steel?
Both are austenitic, but Alloy 800 contains far more nickel and chromium, adds titanium and aluminium, and is designed for oxidation, carburisation and stress corrosion service well above the practical limit of 304.

Q: What is the maximum service temperature of Alloy 800?
The grade is commonly used up to about 600 °C for pressure components and considerably higher for oxidation-resistant furnace parts, depending on the product form and the governing standard.

Q: Can Alloy 800 be welded?
Yes. It is readily welded by gas tungsten arc, plasma arc, gas metal arc and submerged arc processes, with proper cleaning and, where required, a post-weld solution anneal.

Q: Which standards cover Alloy 800 plate and strip?
ASTM B409 covers hot-rolled plate, ASTM B514 covers cold-rolled plate and ASTM B515 covers cold-rolled strip, with matching ASME specifications for pressure service.