Alloy 625 (UNS N06625) plate is one of the reference materials of modern aerospace engineering. It combines high tensile and fatigue strength with oxidation resistance and a corrosion performance that holds up in chlorides, sea water and acidic process streams, and it does so without the need for a precipitation-hardening treatment. This entry summarises the grade, the standards that govern plate supply, the size range normally available, the annealed mechanical requirements and the points that matter when the material is bought for aircraft hardware.
Why Alloy 625 Plate Is Specified in Aerospace Structures
Three properties drive the selection. First, high-temperature strength: the alloy retains useful load-carrying capability in the hot sections of an aircraft, which is why it appears in exhaust systems, ducting, thrust reverser components and engine hardware. Second, fatigue and corrosion fatigue resistance: repeated thermal cycling combined with salt-laden air demands a material that resists both crack initiation and crack growth. Third, fabrication flexibility: plate can be bent, machined and welded into complex assemblies because the grade is supplied annealed and does not depend on a hardening cycle that could distort a finished part.
The alloy is also remarkably tolerant of the thermal and chemical environment at the exhaust end of an aircraft, where hot corrosive gases, condensates and high velocity flow coexist. Designers value the fact that one material can serve both a hot structural function and a corrosion-resisting function, which reduces the number of dissimilar joints in an assembly.
Designation, Standards and Supply Forms
| Item | Reference |
|---|---|
| Common alloy name | Alloy 625 |
| UNS number | N06625 |
| Plate and sheet specification | ASTM B443 / ASME SB-443 |
| Aerospace material specification for sheet, plate and strip | AMS 5599 |
| Rod, bar and forging stock | ASTM B446 / ASME SB-446 |
| European designation | NiCr22Mo9Nb, Werkstoff 2.4856 |
| Delivery condition | Annealed and descaled or pickled, as ordered |
Plate is ordered to the product specification that matches the design authority's requirement. Where a program calls for AMS 5599 rather than ASTM B443, the mechanical and inspection requirements of that aerospace specification take precedence, and the mill should be told at enquiry stage so that testing is planned correctly.
Chemical Composition of UNS N06625 Plate
The composition below is the range specified for the plate grade. The combination of molybdenum and niobium is what separates the alloy from simpler nickel-chromium grades.
| Element | Specified range | Contribution |
|---|---|---|
| Ni | 58.0 min | Matrix; resistance to chloride stress corrosion cracking |
| Cr | 20.0 - 23.0 | Oxidation and oxidising-corrosion resistance |
| Mo | 8.0 - 10.0 | Solid-solution strengthening; pitting and crevice corrosion resistance |
| Nb + Ta | 3.15 - 4.15 | Strengthening; stabilises the structure against sensitisation during welding |
| Fe | 5.0 max | Matrix balance |
| C | 0.10 max | Carbide control |
| Mn | 0.50 max | Deoxidation |
| Si | 0.50 max | Deoxidation; held low for weldability |
| Co | 1.0 max | Controlled residual |
| Al | 0.40 max | Controlled residual |
| Ti | 0.40 max | Controlled residual |
| P | 0.015 max | Residual; controlled for toughness |
| S | 0.015 max | Residual; controlled for hot workability |
Density of the grade is approximately 8.4 grams per cubic centimetre, and the commonly quoted maximum service temperature for the alloy is about 980 degrees Celsius, which is the upper end of the plateau over which it retains useful strength and oxidation resistance.
Plate Size Range and Surface Finish
Plate for aerospace and general industry is normally produced in a standard program that covers both structural and heat-shield thicknesses.
| Parameter | Typical program range |
|---|---|
| Thickness | 3.0 mm to 50.0 mm |
| Width | 50 mm to 2000 mm |
| Length | 50 mm to 6000 mm |
| Surface finish | No. 1, 1D, pickled, or a finish agreed for the application |
| Cutting | Plate can be supplied cut to size, with edge preparation defined by the drawing |
| Packing | Wooden pallet or wooden case with edge protection for transport |
Annealed Mechanical Requirements and Machining Behaviour
Alloy 625 gains its strength from molybdenum and niobium in solid solution, so it is supplied in the annealed condition and does not need artificial aging. The annealed grade is commonly specified with minimum tensile strength of about 827 megapascals, minimum 0.2 percent offset yield strength of about 414 megapascals and minimum elongation of 30 percent, with the understanding that the applicable product specification and thickness govern the exact values printed on the certificate. Cold rolling raises strength further where a temper-rolled condition is required, at some cost in ductility.
For machining, the grade behaves better than many precipitation-hardened nickel alloys. It is prone to chatter because it is stiff and strong, but it does not work harden to the same degree as Alloy 718 (UNS N07718), so a rigid setup with a positive rake tool and generous feed per tooth gives a stable and repeatable cut. Cutting fluid should be plentiful and continuous, because the alloy conducts heat poorly and the tool edge absorbs heat that stays close to the cutting zone. Slow speeds with deep, constant engagement are more productive than high speeds with light passes.
Applications in Airframes and Engines
Engine exhaust systems, tailpipes, liners and heat shields.
Ducting, seals and bracketry in hot zones where thermal fatigue resistance is critical.
Thrust reverser and nacelle components exposed to hot corrosive exhaust gas.
Combustion chamber and turbine section hardware where high-temperature strength is required.
Structural fasteners, fittings and components where high strength and corrosion resistance must coexist.
Outside aerospace the same plate is used for marine and offshore hardware, chemical process vessels and internals, nuclear fuel handling equipment, and sour gas components, which is why the grade is often held in stock for more than one end use.
Quality Documentation for Plate Purchases
Plate for aerospace use is normally released with an inspection certificate that reports heat number, chemical composition, tensile test results and the surface and dimensional checks carried out during finishing. Additional requirements frequently imposed include ultrasonic examination for internal soundness, positive material identification of the finished plate, and grain size or corrosion test evidence where the specification calls for it. Keeping the heat number linked to the finished part is essential for traceability, and plate should be stored indoors on timber dunnage with the heat number preserved so that it can be matched to the certificate at any time.
Frequently Asked Questions
Q: Which grade and UNS number is used for Alloy 625 plate?
Aerospace and general plate is produced from Alloy 625, UNS N06625, with the European designation NiCr22Mo9Nb and Werkstoff number 2.4856.
Q: Which specifications govern the plate?
ASTM B443 and ASME SB-443 cover plate, sheet and strip, AMS 5599 is the aerospace material specification for the same product forms, and ASTM B446 covers rod, bar and forging stock.
Q: Why is the plate supplied annealed rather than aged?
The alloy is strengthened by molybdenum and niobium in solid solution, not by precipitation, so annealing gives the specified strength together with the ductility and toughness needed for forming and welding.
Q: What thickness range is normally available?
A typical production program covers thicknesses from 3.0 mm to 50.0 mm, widths from 50 mm to 2000 mm and lengths from 50 mm to 6000 mm, with No. 1, 1D or pickled finishes.
Q: How does the alloy machine compared with Alloy 718?
It is generally easier to machine because it does not work harden as severely, although chatter is a common problem. Rigid fixturing, positive rake geometry, constant feed and heavy flood cooling give the best results.
Q: What documentation should accompany aerospace plate?
A mill inspection certificate reporting heat number, chemistry, mechanical properties and dimensional checks, supported where required by ultrasonic examination, positive material identification and corrosion or grain size test evidence.