About Inconel 625 pipes for chemical industry

About Inconel 625 pipes for chemical industry
Inconel 625 (Alloy 625) pipe is an essential material in the chemical industry due to its exceptional corrosion resistance and high strength in extreme environments. It is often used to handle highly corrosive chemicals and high temperatures. This nickel-based high-temperature alloy, rich in nickel, chromium, and molybdenum, provides excellent resistance to various corrosion types, including stress corrosion cracking. Its excellent machinability allows for the fabrication of a wide range of components, making it a versatile and durable material for chemical equipment.
What is 625 tubing made of?
Alloy 625 is a nickel-chromium-molybdenum solid solution-strengthened alloy with a nominal chemical composition of 61% nickel, 22% chromium, and 9% molybdenum. It is commonly referred to by the trade name Inconel® 625 and the generic name UNS N06625.

Inconel 625 pipes Grade Standard And Specification
| ASTM Specification | ASTM B444 ASME SB 444 |
|---|---|
| Standard | ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB |
| ASTM B444 inconel 625 Seamless Pipe Size | 4 to 219mm W. T.: 0.5 to 20mm |
| Inconel 625 Welded Pipe Size | 5.0 - 1219.2 mm |
| Inconel WERKSTOFF NR. 2.4856 EFW Pipe size | 5.0 - 1219.2 mm |
| Swg & Bwg | 12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg., |
| Schedule | XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160 |
| Length | Double Random, Single Random, Standard & Cut length Pipe |
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc |
| Form | inconel 625 are available in form of Round, Square, Hollow, Rectangular, Hydraulic, Coiled, Straight Pipes, "U" Shape, Pan Cake Coils etc. |
| Type | Seamless / ERW/ EFW / Welded / Fabricated / CDW / DOM / CEW inconel 625 |
| End | Plain End, Beveled End, Treaded Pipe, Screwed ends |
Alloy 625 Pipes Chemical Structure
| Grade | S | C | Cr2 | Mn | Al-Ti | Si | Fe | Ni | |
| 625 | min. | – | – | 20.0 | – | – | – | – | 58.0 |
| max. | 0.015 | 0.10 | 23.0 | 0.50 | 0.40 | 0.50 | 5.0 | – | |
Inconel 625 Pipes Mechanical Properties Table
| Grade | Elongational (% in 50mm) min | Yield Properties 0.2% Proof (MPa) min | Tensile Properties (MPa) min |
| 625 | 42.5 | Psi – 75,000 , MPa – 517 | Psi – 1,35,000 , MPa -930 |
625 Pipe Applications in the Chemical Industry
Inconel 625 piping is widely used in the chemical processing industry, with the following applications:
Corrosion-Resistant Transportation: Transports corrosive chemicals, acids, and other aggressive fluids that can degrade other materials.
High-Temperature Equipment: Fabricates components for furnaces, incinerators, and other high-temperature equipment within chemical plants.
Specialty Processes: Handles corrosive media in processes such as refining, waste treatment, and biofuel production.
Heat Exchangers: Its excellent strength and corrosion resistance make it suitable for heat exchangers in chemical processes.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications, and we can provide customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneemetal.com