Nov 14, 2024 Leave a message

Datasheet-For-Inconel-601-1-6-(1)-(1).pdf

Inconel 601 Cold Drawn Forged Bar

Inconel 601 Cold Drawn Forged Bar

Chemical Composition Of Inconel 601 Round Bar

Grade

C

Mn

Si

S

Cu

Fe

Ni

Cr

Inconel 601

0.10 max

1.00 max

0.50 max

0.015max

1.00 max

Balance

58.0 – 63.0

21.0 – 25.0

 

Inconel 601 Bright Bars Mechanical Properties

Grade

C

Mn

Si

S

Cu

Fe

Ni

Cr

Inconel 601

0.10 max

1.00 max

0.50 max

0.015max

1.00 max

Balance

58.0 – 63.0

21.0 – 25.0

 

Inconel 601 Forged Bar Physical Properties

Element

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

Inconel 601

8.1 g/cm3

1411 °C (2571 °F)

Psi – 80,000 , MPa – 550

Psi – 30,000 , MPa – 205

30 %

 

Inconel 601 Cold Drawn Round Bar  Equivalent Grades

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

Inconel 601

2.4851

N06601

NCF 601

NA 49

XH60BT

NC23FeA

NiCr23Fe

Send Inquiry