Nov 13, 2024 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Inconel 600 Bright Annealed Tube

Inconel 600 Bright Annealed Tube

Chemical Composition, %

Ni + Co Cr Fe C Mn S Si Cu

72.0 min

14.0-17.0

6.0-10.0

.15 max

1.00 max

.015 max

.50 max

.50 max

 

Mechanical Properties

Typical room temperature Tensile Properties of Annealed Material

Product Form Condition Tensile (ksi) .2% Yield (ksi) Elongation (%) Hardness (HRB)

Rod & Bar

Cold-Drawn

80-100

25-50

35-55

65-85

Rod & Bar

Hot-Finished

80-100

30-50

35-55

65-85

Tube & Pipe

Hot-Finished

75-100

30-50

35-55

–

Tube & Pipe

Hot-Finished

80-100

25-50

35-55

88 Max

Plate

Hot-Rolled

80-105

30-50

35-55

65-85

Sheet

Cold-Drawn

80-100

30-45

35-55

88 Max

 

Specifications of Inconel 600 include the following:

Rods, bars, wires Forgings Plates, sheets and strips Seamless pipes and tubes Welded pipe and tube Accessories

ASTM B 166/ASME SB 166

ASTM B 564/ASME SB 564

ASTM B 168/ASME SB 168

ASTM B 167/ASME SB 167, ASTM B 163/ASME SB 163

ASTM B 516/ASME SB 516, ASTM B 517/ASME SB 517

ASTM B 366/ASME SB 366

Send Inquiry