Inconel 600 vs 601: What's the Difference
 

Gnee Steel

 

Inconel 600 vs 601: What's the Difference

Inconel 600 is primarily composed of nickel and chromium, with trace amounts of iron, manganese, carbon, sulfur, silicon, and other elements added to achieve specific properties. Inconel 601 adds aluminum to this composition, giving it higher strength at high temperatures than Inconel 600.

Inconel 600 vs 601: What's the Difference

Gnee Steel

 

What are the applications of Inconel 601?

The properties of Inconel 601 alloy make it a widely used material in fields such as heat treatment, chemical processing, pollution control, aerospace, and power generation. 601 alloy is a standard structural material for various heat treatment equipment.

Inconel 601

Chemical Composition

Element Inconel Alloy 600 Inconel Alloy 601
Nickel (Ni) 72-76% 58-63%
Chromium (Cr) 14-17% 22-26%
Iron (Fe) Balance Balance
Molybdenum (Mo) None None
Carbon (C) ≤0.15% ≤0.10%
Aluminum (Al) None 1.0-1.5%

 

Mechanical Properties

Property Inconel Alloy 600 Inconel Alloy 601
Yield Strength (MPa) 200 – 310 250 – 450
Ultimate Tensile Strength (MPa) 450 – 700 550 – 750
Elongation (%) 30% (min) 30% (min)
Hardness (Rockwell B) 80-100 85-95

 

High-Temperature Performance

Feature Inconel Alloy 600 Inconel Alloy 601
Service Temperature Up to 1,900°F (1,038°C) Up to 2,100°F (1,149°C)
Oxidation Resistance Good Excellent
Creep Resistance Moderate Very good

 

Corrosion Resistance

Corrosion Type Inconel Alloy 600 Inconel Alloy 601
General Corrosion Very good Good
Pitting Corrosion Good Very good
Stress Corrosion Cracking Moderate Excellent
Acid Resistance Good in non-oxidizing acids Excellent, even in high-temperature environments

 

Weldability Comparison

Feature Inconel Alloy 600 Inconel Alloy 601
General Weldability Good; usually does not require preheating Good; may require preheating
Post-Weld Heat Treatment Generally not required Not usually required
Filler Material ERNi 600 ERNi 601

 

Typical Applications

Application Area Inconel Alloy 600 Inconel Alloy 601
Chemical Processing Heat treating equipment, reactors Heat exchangers in chemical plants
Aerospace Gas turbine components High-temperature components
Oil and Gas Industry Oil refining systems Elevated temperature applications
Power Generation Boiler tubes Superheaters and reheaters
Industrial Furnaces Furnaces and kiln components Furnace components for enhanced stability

 

Summary of Differences

Feature Inconel Alloy 600 Inconel Alloy 601
Nickel Content 72-76% 58-63%
Chromium Content 14-17% 22-26%
Temperature Resistance Up to 1,900°F (1,038°C) Up to 2,100°F (1,149°C)
Oxidation Resistance Good Excellent
Applications Suited for chemical processing and oil refining Preferred for high-temperature applications

 

Why Choose Gnee Nickel Alloy (Supplier Example)?

✅ Large stock of Incoloy alloy tubes/bars/plates/fittings/coils, fast shipping.

✅ Factory direct sales, highly competitive prices, excellent value for money.

✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical property certificate.

✅ Value-added services: slitting, cutting, polishing, surface treatment.

✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.

Email: ss@gneemetal.com

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600/601 alloy, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness: 0.1 to 100 mm; width: 10-2500 mm); strips; alloy round bars (diameter: 3-800 mm); flat bars (thickness: 2-100 mm; width: 10-500 mm); hexagonal bars (size: 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with Inconel 600/601 alloy products that meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600/601, pipes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel
Inconel 600 vs 601: What's the Difference
Inconel 600 vs 601: What's the Difference
Inconel 600 vs 601 Alloy
Inconel 600 vs 601 Alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry