Sheet and Plate Weight Chart
| Plate Thickness (mm) | Weight (kg/m) | kg/meter (width 1200mm) | kg/meter (width 1500mm) | kg/meter (width 1800mm) | kg/meter (width 2400mm) |
|---|---|---|---|---|---|
| 3 | 23.55 | 28.3 | 35.3 | 42.4 | 56.5 |
| 4 | 31.4 | 37.7 | 47.1 | 56.5 | 75.4 |
| 5 | 39.25 | 47.1 | 58.9 | 70.7 | 94.2 |
| 6 | 47.1 | 56.5 | 70.7 | 84.8 | 113 |
| 8 | 62.8 | 75.4 | 94.2 | 113 | 150.7 |
| 10 | 78.5 | 94 | 118 | 141 | 188 |
| 12 | 94.2 | 113 | 141 | 170 | 226 |
| 16 | 125.6 | 151 | 188 | 226 | 301 |
| 20 | 157 | 188 | 236 | 283 | 377 |
| 22 | 172.7 | 207 | 259 | 311 | 415 |
| 25 | 196.25 | 236 | 294 | 353 | 471 |
| 28 | 219.8 | 264 | 330 | 396 | 528 |
| 32 | 251.2 | 301 | 377 | 452 | 603 |
| 36 | 282.6 | 339 | 424 | 509 | 678 |
| 40 | 314 | 377 | 471 | 565 | 754 |
| 45 | 353.25 | 424 | 530 | 636 | 848 |
| 50 | 392.5 | 471 | 589 | 707 | 942 |
| 55 | 431.75 | 518 | 648 | 777 | 1036 |
| 60 | 471 | 565 | 707 | 848 | 1130 |
| 65 | 510 | 612 | 765 | 918 | 1224 |
| 70 | 549.5 | 659 | 824 | 989 | 1319 |
| 75 | 588.75 | 707 | 883 | 1060 | 1413 |
| 80 | 628 | 754 | 942 | 1130 | 1507 |
| 90 | 706.5 | 848 | 1060 | 1272 | 1696 |
| 100 | 785 | 942 | 1178 | 1413 | 1884 |
Gnee Steel also supplies custom Inconel 600 products in various sizes and specifications. Please send us your drawings for a quote!