Inconel 600/690 round bar counterweight

Inconel 600 round bar weight chart, Nickel 600 round bar weight per meter, Inconel 600 Alloy round bar weight chart, 600 alloy bar weight chart.

 

Inconel 600 Round Bar Tolerance Chart

Dia Weight Dia Weight
(mm) per metre (kg) (in) per metre (kg)
3mm 0.06 1/8″ 0.06
4mm 0.10 3/16″ 0.14
5mm 0.16 1/4″ 0.25
6mm 0.22 5/16″ 0.39
7mm 0.30 3/8″ 0.56
8mm 0.40 7/16″ 0.77
10mm 0.62 1/2″ 1.00
12mm 0.89 9/16″ 1.22
14mm 1.22 5/8″ 1.56
15mm 1.40 11/16″ 1.89
16mm 1.59 3/4″ 2.25
18mm 2.01 7/8″ 3.07
20mm 2.48 1″ 4.03
22mm 3.00    
24mm 3.57    
25mm 3.88    

Inconel 600 bar stock supplier. Nickel 600 metric round bar weight chart, 12mm round bar weight chart.