Jan 30, 2024 Leave a message

Hastelloy C22 (UNS N06022): Properties and Applications

Alloy Overview

Hastelloy C22 (UNS N06022) is a nickel-chromium-molybdenum-tungsten corrosion-resistant alloy. It is one of the few materials that delivers reliable resistance to oxidizing, reducing and mixed acidic corrosive media simultaneously. The grade is widely produced in plate, sheet, bar, pipe, forging and welding filler forms for severe corrosive environments across the chemical, environmental and energy industries.

Chemical Composition

Typical composition limits for UNS N06022, in weight percent, are nickel as balance, chromium 20.0-22.5%, molybdenum 12.5-14.5%, tungsten 2.5-3.5%, iron 2.0-6.0%, carbon maximum 0.015%, silicon maximum 0.08%, manganese maximum 0.50%, phosphorus maximum 0.020% and sulfur maximum 0.020%. Actual chemical acceptance must comply with ASTM material standards and the mill test certificate for each heat.

Physical and Mechanical Properties

Typical annealed physical properties include density of 8.69 g/cm³ (0.314 lb/in³), melting range of approximately 1330-1357°C, coefficient of linear thermal expansion of 12.8 µm/m·°C from 20 to 100°C, thermal conductivity of 9.8 W/m·K at 20°C, and electrical resistivity of 114 µΩ·cm at room temperature. Typical room-temperature mechanical properties in the annealed condition include tensile strength of at least 690 MPa, 0.2% offset yield strength of at least 283 MPa, elongation of at least 30% over a 50 mm gauge, and hardness of HRB 100 maximum. Mechanical performance varies with product thickness, forming process and heat treatment, and final inspection follows the official material specification.

Metallurgical Microstructure

After proper solution annealing, Hastelloy C22 exhibits a fully austenitic single-phase matrix. Controlled low carbon content minimizes intergranular carbide precipitation during welding or thermal exposure, stabilizing corrosion resistance in welded assemblies. Unlike duplex or precipitation-hardening alloys, this grade does not rely on intermetallic hardening phases; its corrosion resistance originates from the balanced chromium, molybdenum and tungsten alloying design.

Corrosion Resistance Characteristics

Hastelloy C22 provides comprehensive resistance to oxidizing media such as nitric acid, ferric chloride and cupric chloride solutions; reducing media such as dilute sulfuric and hydrochloric acids; mixed acid systems and flue gas desulfurization scrubber liquors; and pitting, crevice corrosion and stress corrosion cracking in chloride-containing brines. It performs better than Hastelloy C276 in many oxidizing mixed corrosive environments, which makes it a preferred selection for complex multi-media service.

Industrial Applications

Typical applications include flue gas desulfurization scrubbers and internal components, waste incineration boiler liners, mixed acid chemical reactors, chlor-alkali filter housings, electroplating bath linings, hazardous waste treatment evaporators, offshore produced water treatment equipment, pharmaceutical corrosive synthesis reactors, pulp and paper bleach plant equipment, and welded corrosion-resistant piping modules. Common product forms are plate, sheet, strip, round bar, flat bar, hex bar, seamless pipe, welded tube, pipe fittings, forgings, flanges and welding wire, normally supplied in the solution-annealed and pickled condition with non-destructive testing on request.

FAQ

Q: What is Hastelloy C22 (UNS N06022)?

A: It is a nickel-chromium-molybdenum-tungsten alloy offering outstanding resistance to oxidizing, reducing and mixed acidic corrosive media, widely used in severe chemical service.

Q: What is the hardness of annealed Hastelloy C22?

A: Hardness in the annealed condition is HRB 100 maximum; final acceptance follows the official material specification for each product form.

Q: How does C22 compare with C276?

A: C22 performs better than C276 in many oxidizing mixed corrosive environments, while both offer excellent resistance to pitting, crevice corrosion and stress corrosion cracking.

Q: What standards cover Hastelloy C22 products?

A: Common standards include ASTM B575 for plate, sheet and strip, B619 for welded pipe, and B464 for welded tube, among related ASTM/ASME specifications.

Q: Is Hastelloy C22 weldable?

A: Yes, and its low carbon content minimizes carbide precipitation in the heat-affected zone, preserving corrosion resistance in welded assemblies.

Q: What forms of C22 are available?

A: Plate, sheet, strip, round bar, flat bar, hex bar, seamless pipe, welded tube, pipe fittings, forgings, flanges and welding wire and electrodes.