Hastelloy C22: Introduction, Corrosion Resistance and Properties

Overview of Hastelloy C22

Hastelloy C22 is a versatile nickel-chromium-molybdenum-tungsten alloy with better overall corrosion resistance than other existing nickel-chromium-molybdenum alloys, including C-276, Alloy C-4 and Alloy 625. The chromium, molybdenum and tungsten contents are balanced for stability, giving the alloy high corrosion resistance and good thermal stability. It is designated UNS N06022 and is also known as Alloy 22.

Chemical Composition

The nominal composition of Alloy C-22 is: nickel balance, chromium 20.0-22.5%, iron 2.0-6.0%, molybdenum 12.5-14.5%, tungsten 2.5-3.5%, carbon 0.015% max, manganese 0.50% max, silicon 0.08% max, phosphorus 0.02% max and vanadium 0.02% max. The high chromium content helps the alloy form a thick, stable protective layer that significantly improves corrosion resistance in oxidizing environments, while molybdenum and tungsten support resistance to reducing acids.

Physical and Mechanical Properties

Alloy C-22 has a density of about 8.9 g/cm³ and a melting range of about 1325-1370°C. In the solution-annealed condition at room temperature, minimum mechanical properties are about 690 MPa tensile strength, 283 MPa 0.2% yield strength and 40% elongation. The alloy has high strength, good ductility and hardness, and is easy to hot and cold form and weld. Because yield strength is higher than C-276, engineering design can reduce wall thickness, saving material and cost.

Corrosion Resistance

C-22 resists pitting, crevice corrosion, intergranular corrosion and stress corrosion. It is one of the few materials that resists wet chlorine, hypochlorite and chlorine dioxide solutions, and it has significant resistance to high-concentration chloride salt solutions such as ferric chloride and copper chloride. The alloy resists oxidizing acids such as nitric acid and, thanks to molybdenum and tungsten, reducing acids such as dilute sulfuric and hydrochloric acid. Because of the low carbon content and balanced alloy ratio, the heat-affected zone after welding is not sensitive to medium-temperature sensitization, and chromium carbides and intermetallic compounds do not readily precipitate at grain boundaries. The alloy is therefore suitable for many chemical processes in the welded state and is commonly used as steel lining in flue gas desulfurization systems.

Applications and Welding

C-22 is suited to chemical process industries containing oxidizing and reducing media, and to environments where conditions fluctuate between the two, such as hydrochloric and sulfuric acid solutions mixed with strong oxidizing ions. When joining C-22 to stainless steel or nickel alloys, or for overlay welding on steel, filler metal of the ERNiCrMo-10 classification is commonly used so that the surfacing layer serves as the corrosion-resistant layer or transition layer. For nitrogen-containing duplex or austenitic stainless steels, niobium-free welding consumables can be used to avoid precipitation of niobium-nitrogen compounds that would affect post-weld properties.

FAQ

Q: What is Hastelloy C22?

A: It is a nickel-chromium-molybdenum-tungsten alloy, UNS N06022, with balanced composition for resistance to both oxidizing and reducing corrosive media.

Q: How does C-22 compare with C-276?

A: C-22 offers better overall corrosion resistance, especially in oxidizing environments, with higher yield strength and similar price because of comparable ingredients and production routes.

Q: Is C-22 resistant to wet chlorine?

A: Yes, it is one of the few materials resistant to wet chlorine, hypochlorite and chlorine dioxide solutions.

Q: What are the density and melting range?

A: About 8.9 g/cm³ density and a melting range of about 1325-1370°C.

Q: Can C-22 be used in the welded condition?

A: Yes, its low carbon content and balanced composition make the heat-affected zone resistant to sensitization, so it suits many chemical processes in the welded state.

Q: What filler metal is used for welding C-22?

A: Filler metal of the ERNiCrMo-10 classification is commonly specified for joining and overlay applications.