Hastelloy C276 Butt Welding Pipe Fittings Dimension Table

ASME b16.9 Fittings
Normal Pipe Size
ANSI b16 9 Pipe Fitting O
D Y
Wall Thickness T
(Pipe Elbow Sch.)
LR 45 Deg Elbows Centre to Face B SR 45 Deg Elbows
Weight
LR 90 Deg Elbows Centre to Face A LR 90 Deg Elbows Weight In Below SR 90 Deg Elbows Centre to Face A SR 90 Deg Elbows Weight In Below
millimeter inch. millimeter millimeter Schedule millimeter kilogram millimeter kilogram millimeter kilogram
15 1/2" 21.3 2.78 STD 15.9 0.04 38.1 0.08 – –
      3.73 X.S 15.9 0.05 38.1 0.10 – –
20 3/4" 26.7 2.87 STD 11.1 0.04 28.6 0.08 – –
      3.91 X.S 11.1 0.05 28.6 0.11 – –
25 1" 33.4 3.38 STD 22.2 0.09 38.1 0.15 25.4 0.11
      4.55 X.S 22.2 0.11 38.1 0.19 25.4 0.14
32 11/4" 42.2 3.56 STD 25.4 0.14 47.6 0.28 31.75 0.18
      4.85 X.S 25.4 0.2 47.6 0.39 31.75 0.24
40 11/2" 48.3 3.68 STD 28.6 0.2 57.1 0.4 38.1 0.26
      5.08 X.S 28.6 0.25 57.1 0.5 38.1 0.35
50 2" 60.3 3.91 STD 34.9 0.36 76.2 0.72 50.8 0.5
      5.54 X.S 34.9 0.5 76.2 1.0 50.8 0.68
65 21/2" 73.0 5.16 STD 44.4 0.73 95.2 1.46 63.5 0.95
      7.01 X.S 44.4 0.91 95.2 1.82 63.5 1.27
80 3" 88.9 5.49 STD 50.8 1.1 114.3 2.18 76.2 1.45
      7.62 X.S 50.8 1.45 114.3 2.86 76.2 1.95
100 4" 114.3 6.02 STD 63.5 2.1 152.4 4.2 101.6 2.8
      8.56 X.S 63.5 2.9 152.4 5.7 101.6 3.9
125 5" 141.3 6.65 STD 79.4 3.4 190.0 6.8 127.0 4.8
      9.5 X.S 79.4 5.0 190.0 10.0 127.0 6.5
150 6" 168.3 7.11 STD 95.2 5.1 229.0 10.1 152.4 6.8
      10.97 X.S 95.2 7.7 229.0 15.3 152.4 10.2
200 8" 219.1 8.18 STD 127.0 10.2 305.0 20.4 203.0 13.6
      12.7 X.S 127.0 15.5 305.0 30.9 203.0 20.9
250 10" 273.9 9.27 STD 159.0 18.1 381.0 36.1 254.0 24.1
      12.7 X.S 159.0 24.4 381.0 48.8 254.0 32.5
300 12" 323.9 9.52 STD 190.0 26.6 457.0 53.1 305.0 35.4
      12.7 X.S 190.0 35.0 457.0 70.0 305.0 46.7
350 14" 355.6 9.52 STD 222.0 34.1 533.0 68.1 356.0 45.4
      12.7 X.S 222.0 45.0 533.0 90.0 356.0 60.0
400 16" 406.4 9.52 STD 254.0 45.0 610.0 89.3 406.0 59.5
      12.7 X.S 254.0 59.0 610.0 118.0 406.0 78.7
450 18" 457.0 9.52 STD 286.0 56.5 686.0 113.0 457.0 75.6
      12.7 X.S 286.0 75.0 686.0 150.0 457.0 100.0
500 20" 508.0 9.52 STD 318.0 85.0 762.0 140.0 508.0 93.5
      12.7 X.S 318.0 112.5 762.0 186.0 508.0 124.0
600 24" 610.00 9.52 STD 381.0 101.5 914.0 203.0 610.0 135.0
      12.7 X.S 381.0 134.5 914.0 269.0 610.0 179.0