Hastelloy C276 pipe fitting tolerances

Hastelloy C276 pipe fittings, tolerances for butt welded pipe fittings, tolerance table for C276 pipe fittings (mm), dimensions of alloy C276 butt welded straight-through tee.

 

Hastelloy C276 pipe fittings size table

All Fittings 90, 45 Elbows and Tees Reducers Caps 180 Returns Angularity Tolerance
Nominal Pipe Size Outside Diameter at Bevel Inside Diameter at End Wall Thickness Center to End Dimension Overall Length Overall Length Center to Center Dimension Back to face Dimension Alignment of Ends Nominal Pipe Size off Angle off Plane
(in) D   t A.B.C.M H E O K U (in) Q P
1/2to 21/2 +1.52-0.76 0.76 Not Less Than 87.5% of Nominal Thickness 1.52 1.52 3.05 6.35 6.35 0.76 1/2 to 4 0.76 1.51
3 to 31/2 1.52 1.52 1.52 1.52 3.05 6.35 6.35 0.75 5 to 8 1.52 3.05
4 1.52 1.52 1.52 1.52 3.05 6.35 6.36 0.76 10 to 12 2.29 4.83
5 to 8 +2.29-1.52 1.52 1.52 1.52 6.35 6.35 6.35 0.76 14 to 16 2.29 6.35
10 to 18 +4.06-3.05 3.05 2.29 2.29 6.35 9.65 6.35 1.52 18 to 24 3.05 9.65
20 to 24 +6.35-4.83 4.83 2.29 2.29 6.35 9.65 6.35 1.52 26 to 30 4.83 9.65
26 to 30 +6.35-4.83 4.83 3.05 4.83 9.65 – – – 32 to 36 4.83 12.7
32 to 36 +6.35-4.83 4.83 4.83 4.83 9.65 – – –      

 

Gnee Steel also supplies custom Hastelloy C276 pipe fittings in various sizes and specifications. Please send us your drawings for a quote! 