Hastelloy C22 alloy is suitable for various chemical process industries containing oxidizing and reducing media. The higher content of molybdenum and chromium makes the alloy resistant to chloride ion corrosion, and the tungsten element further improves its corrosion resistance.

Hastelloy C-22 (UNS N06022/W N 2.4602)
| alloy |
% |
Nickel | Chromium | Molybdenum | Iron | Tungsten | Cobalt | Carbon | Manganese | Silicon | Vanadium | Phosphorus | Sulfur |
|
C22 |
min |
- |
20.0 |
12.5 |
2 |
2.5 |
- |
- |
- |
- |
- |
- |
- |
|
- |
max |
- |
22.5 |
14.5 |
6 |
3.5 |
2.5 |
0.015 |
0.5 |
0.08 |
0.35 |
0.02 |
0.02 |
Physical properties
| density |
8.9 g/cm3 |
| Melting point |
1325-1370 ℃ |
Minimum mechanical properties of Hastelloy C-22 alloy at room temperature:
| Alloy and state |
tensile strength Rm N/mm2 |
Yield Strength RP0.2N/mm2 |
Elongation A5 % |
|
Hastelloy C22 |
690 |
283 |
40 |
Application areas of Hastelloy C22:
Hastelloy C22 is widely used in the chemical and petrochemical fields, especially for components and catalytic systems that come into contact with chloride-containing organic matter. In addition, it also performs very well in high temperature, inorganic and organic acids mixed with impurities, and seawater corrosion environments.
Comparison with Hastelloy C4:
Compared with Hastelloy C4, Hastelloy C22 has a wider range of corrosion resistance, including better resistance to pitting, crevice corrosion, and stress corrosion cracking. Therefore, according to the specific industrial application requirements, the appropriate Hastelloy alloy can be selected to ensure that the material can meet the requirements of the specific process.