Dec 12, 2024 Leave a message

Hastelloy® C-4 UNS N06455 pipe

Hastelloy C-4 alloy has excellent corrosion resistance and thermal stability, and is suitable for corrosive environments and high-temperature applications such as flue gas desulfurization and acetic acid production.

Hastelloy C-4 alloy

Process performance and requirements:
During the heat treatment process, the alloy should be avoided from contact with low-melting-point metals such as sulfur, phosphorus, and lead to maintain its stability. The hot working temperature range should be between 1080℃ and 900℃, and water cooling or other rapid cooling methods are recommended for cooling.

Hastelloy® C-4 UNS N06455

Material brand and identification:
Hastelloy C-4 (N06455)
German brand: W.Nr. 2.4610
American brand: UNS N06455

 

Physical properties:
Density: 8.64g/cm³
Melting point: 1350-1400℃
Mechanical properties (at room temperature):
Tensile strength Rm: 783 N/mm²
Yield strength Rp0.2: 365 N/mm²
Elongation A: 55%

 

Overview of characteristics and application areas:
Hastelloy C-4 alloy is an austenitic low-carbon nickel-molybdenum-chromium alloy. Compared with other similar alloys (such as Nicrofer 6616 hMo), its unique chemical composition (low carbon, silicon, iron, and tungsten content) gives it excellent stability in the range of 650-1040℃.


High temperature characteristics and uses: Hastelloy C-4 (Ni-Cr-Mo) maintains excellent thermal stability and toughness in high temperature environments, and has good resistance to stress corrosion cracking and oxidizing atmospheres at high temperatures. Therefore, it is particularly suitable for corrosive environments such as mineral acids, chlorine-containing media, acetic acid, seawater and salt water. It has a wide operating temperature range from -200℃ to +400℃, and has good structural stability and can be used directly after welding.

 

Send Inquiry

whatsapp

Phone

E-mail