Hastelloy C-22 is a solid solution strengthened nickel-based high temperature and high strength alloy. At room temperature, its yield strength is about 400MPa and its tensile strength is about 690MPa. At high temperatures, its yield strength and tensile strength are both improved, up to about 1000°C.

The physical properties of Hastelloy C-22 mainly include:
Density: about 8.69~8.9 g/cm³.
Melting point: about 1300~1370°C.
Thermal expansion coefficient: varies with temperature, but usually in the range of 12~14 × 10^-6 /°C.
Thermal conductivity: about 11 W/(m·K) at room temperature.
Specific heat capacity: about 0.49~0.414 J/g·°C (different data vary slightly).
Elastic modulus: about 200~206 GPa.
Corrosion resistance
Hastelloy C-22 has excellent resistance to various corrosive environments, including wet chlorine, nitric acid, oxidizing acid mixtures of chloride ions, as well as formic acid, acetic acid, acetic anhydride, seawater and salt solutions. It is one of the only materials that can resist corrosion from wet chlorine, hypochlorite and chlorine dioxide solutions.
Manufacturing process
The manufacturing process of Hastelloy C-22 includes raw material preparation, smelting, casting, forging and rolling, heat treatment and other steps. Among them, heat treatment usually adopts solid solution treatment, and the heating temperature should be between 1150℃ and 1200℃, and it should be kept at this temperature for a long enough time to ensure the uniformity of the material inside.

Application field
Chemical industry: used to manufacture key equipment such as reactors, heat exchangers, pumps and valves.
Marine industry: used to manufacture components of ships and offshore platforms, which can resist corrosion from seawater.
Papermaking industry: used to manufacture bleaching equipment and chemical processing equipment.
Energy industry: used to manufacture components in nuclear reactors, adapting to high temperature and high pressure working environments.
Aerospace field: used to manufacture engine components and high-temperature components to meet the requirements of high strength and corrosion resistance of materials.