Floating iron powder or embedded iron will corrode stainless steel

On any surface, free iron rusts and corrodes stainless steel. Therefore, it must be cleared. Float powder can generally be removed along with the dust. Some have strong adhesion and must be treated according to the embedded iron. In addition to dust, there are many sources of surface iron, including cleaning with ordinary carbon steel wire brushes and shot blasting with sand, glass beads or other abrasives previously used on plain carbon steel, low alloy steel or cast iron parts, or polishing the aforementioned non-stainless steel products near stainless steel parts and equipment. Iron on wire ropes, spreader and workbench surfaces can easily become embedded or stain surfaces if the stainless steel is not protected during unloading or lifting. Order requirements and post-production inspections can prevent and detect the presence of free iron, ASTM standard A380[3] specifies the rust test method for the inspection of iron or steel particles on the surface of stainless steel. This test should be used when it is required that there must be absolutely no iron present. If the results are satisfactory, wash the surface with clean pure water or nitric acid until the dark blue is completely gone. As indicated in standard A380[3], if the rust test solution cannot be completely removed, it is not recommended to use this test method on the process surface of the equipment, i.e. the direct contact surface used to produce human consumer goods. A relatively simple test method is to be exposed to water for 12 to 24 hours to check whether there are rust spots. Such tests are less sensitive and time-consuming. These are detection tests, not cleanup methods. If iron is found to be present, it must be cleaned using the chemical and electrochemical methods described below.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry