Dec 03, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Differences between Nickel 600 and EN 1.4941 stainless steel

 
Differences between Nickel 600 and EN 1.4941 stainless steel
Differences between Nickel 600 and EN 14941 stainless steel
01

Differences between Nickel 600 and EN 1.4941 stainless steel

Nickel 600 is a nickel alloy with a high nickel content (approximately 72%) and excellent corrosion resistance, while EN 1.4941 is an iron-based stainless steel. The main difference between the two lies in their base metals (nickel versus iron). Nickel 600 has superior high-temperature resistance and a wider range of corrosion resistance, thus it is more expensive and more suitable for specialized applications, while EN 1.4941 is more common and economical.

02

What is the equivalent material of Inconel 600 casting alloy?

Inconel 600, equivalent to UNS N06600, is a high-strength nickel-chromium alloy. It is known for its excellent corrosion resistance, strength, and superior performance even at extreme temperatures. This alloy contains not only nickel and chromium, but also iron and many other different elements.

Inconel 600
 

Composition and classification of nickel 600 and EN 1.4941 stainless steel

Feature Nickel 600 EN 1.4941
Alloy Type Nickel-chromium alloy (High-nickel alloy) Iron-based stainless steel (Ferroalloy)
Base Metal Nickel Iron
Nickel Content 72-78% Varies (typically ~10-12% for 1.4941)
Chromium Content 14-17% ~17-19% (typical)
Iron Content 6-10% Balance (typically ~65-70%)
Material Category High-nickel superalloy Austenitic stainless steel

 

Comparison of the properties and performance of nickel 600 and EN 1.4941 stainless steel

Property Nickel 600 Stainless Steel EN 1.4941
Corrosion Resistance Extremely high; resistant to various corrosive media, alkaline solutions, dry chlorine, and hydrogen chloride at high temperatures Generally good but less resistant to certain aggressive chemicals and high-temperature chlorides
Temperature Resistance Excellent; strength remains stable over a wide temperature range; suitable for extreme high-temperature environments Performance degrades at high temperatures; not suitable for extreme conditions where nickel alloys excel
Strength at Low Temperatures High, but some stainless steels may have higher strength at lower temperatures Often higher than nickel 600 at ambient and low temperatures
Strength at High Temperatures Retains strength better as temperature increases; superior high-temperature mechanical properties Loses strength significantly as temperature rises
Suitability for Extreme Environments Highly suitable for high-temperature, corrosive, and alkaline conditions Limited suitability for extreme high-temperature or highly corrosive environments

 

Applications and costs of Nickel 600 and EN 1.4941 stainless steel

Aspect Nickel 600 EN 1.4941
Applications Chemical processing, aerospace, power generation (demanding environments) Construction, food processing, general-purpose structural components
Cost Generally more expensive More cost-effective

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 

About Gnee Steel

Gnee Steel is a supplier of Nickel 600 alloy, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness: 0.1 to 100 mm; width: 10-2500 mm); strips; alloy round bars (diameter: 3-800 mm); flat bars (thickness: 2-100 mm; width: 10-500 mm); hexagonal bars (size: 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with Nickel 600 alloy products that meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Nickel 600, pipes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry