Corrosion-resistant alloy Inconel 617 (UNS N06617)

Corrosion-resistant alloy Inconel 617 (UNS N06617)

 

Corrosion-resistant alloy Inconel 617 (UNS N06617)
Material grade: Inconel 617 (UNS N06617)

German brand: W.Nr.2.4663

DIN grade:NiCr23Co12Mo

US grade: UNS N06617

ISO grade: NiCr22Co12Mo9

Inconel 617 is a nickel-chromium-cobalt-molybdenum alloy with excellent mechanical properties at high temperatures. The alloy is resistant to high-temperature corrosion properties such as oxidation and carbonization.

Inconel 617 has the following features:

●Excellent instantaneous and long-term mechanical properties at high temperatures up to 1100℃
●High oxidation resistance at 1100℃

●High carbonation resistance at 1100℃

●Good welding performance

Inconel 617 physical properties:

Typical physical properties at room temperature and high temperature

Density: ρ=8.4g/cm3

Melting temperature range: 1330~1380℃

Inconel 617 metallographic structure:

Inconel 617 alloy has a face-centered cubic lattice structure and has good crystal phase stability. Excellent high-temperature strength is achieved through solid solution hardening, and the alloy does not undergo age hardening.

Corrosion-resistant alloy Inconel 617 (UNS N06617)

Corrosion-resistant alloy Inconel 617 (UNS N06617)

Inconel 617 corrosion and heat resistance properties:

Inconel 617 alloy has excellent corrosion resistance in hot corrosion fields such as sulfide environments, especially oxidation and carbonization environments that cycle up to 1100°C. These corrosion resistance properties, combined with excellent mechanical properties, make this alloy particularly suitable for use in high-temperature applications.

In addition, the higher nickel, chromium, and molybdenum contents make the alloy have good corrosion resistance in most corrosive media.

Inconel 617 Application:

Inconel 617 is suitable for use in high temperature and extremely high mechanical stress applications. The recommended operating temperature does not exceed 1000°C. At the same time, Inconel 617 is suitable for applications where weight reduction is required, such as processing of thin-walled structural parts.

● Industrial and aerospace turbine components

● Air heater

● Muffle Tank and Radiation Pavilion

● High temperature heat exchangers, valves and springs

● High-temperature gas cooling nuclear reactor, such as high-temperature components of nuclear reactor-helium/helium medium heat exchanger

● Chemical equipment

● Spiral tubes and pipes in the petrochemical industry

Inconel 617 Processing and Heat Treatment

Inconel 617 alloy is easy to process in a variety of hot and cold processes, but requires high-power equipment due to its high strength.

Inconel 617 alloy has excellent welding properties and can be welded using various welding methods.

Inconel 617 warm-up:

The surface of the workpiece must be cleaned before and during the heating process to keep the surface clean. Inconel 617 alloy will become brittle if the heating environment contains sulfur, phosphorus, lead or other low melting point metals. Impurities come from marking paint, chalk, lubricating oil, water, fuel, etc. The sulfur content of fuel should be low. For example, the impurity content of liquefied petroleum gas and natural gas should be less than 0.1%, the sulfur content of city gas should be less than 0.25g/m3, and the sulfur content of petroleum gas should be less than 0.5%.

The heated electric furnace should preferably have a more precise temperature control capability. The furnace gas must be neutral or weakly oxidizing, and the furnace gas composition should be prevented from fluctuating between oxidizing and reducing properties. The heating flame cannot be directed toward the workpiece.

During all heating processes, materials must be added to the heated furnace.
Inconel 617 thermal processing:

Due to the very high thermal intensity, considerable processing forces are required during thermal processing.

The suitable thermal processing temperature for Inconel 617 alloy is 1200-950°C. The cooling method can be water quenching or other rapid cooling methods. The material must be entered into the heating furnace when it reaches the maximum furnace temperature.

Inconel 617 cold working:

Cold working should be carried out after annealing. The work hardening rate of Inconel 617 is greater than austenitic stainless steel, so the processing equipment should be adjusted accordingly, and there should be an intermediate annealing process during the cold working process.

When the cold deformation is greater than 10% or for materials with application temperatures above 900°C, the cold deformation is greater than 5%, final solution annealing is required.
Inconel 617 heat treatment:

In order to obtain appropriate properties, the solution treatment temperature is 1150℃-1200℃, and it must be water quenched to obtain maximum creep resistance. If the thickness is less than 1.5mm, it can also be quickly air-cooled.

Stress relief annealing temperatures can reach 870°C.

During all heat treatments, pay attention to the matters mentioned earlier about maintaining cleanliness.
Inconel 617 polishing:

Oxides near the welds of Inconel 617 workpieces are more difficult to remove than those of stainless steel. Mechanical or chemical methods can be used

When using mechanical methods, avoid metal contamination and high surface deformation. Before pickling in a mixed acid of nitric and hydrofluoric acid, oxides should also be removed with sandpaper or pre-treated in a salt bath.

Inconel 617 machining:

The machining of Inconel 617 needs to be carried out after solution treatment. To take into account the work hardening of the material, Inconel 617 must use lower surface cutting speeds and heavy feeds than low-alloy standard austenitic stainless steel.

 