Jan 21, 2026 Leave a message

Datasheet-For-Inconel-601-1-6-(1)-(1).pdf

Comprehensive specifications for Inconel 601 Alloy Rings

 
Comprehensive specifications for Inconel 601 Alloy Rings
 
Comprehensive Specifications For Inconel 601 Alloy Rings.

Comprehensive specifications for Inconel 601 Alloy Rings

Inconel 601 (UNS N06601) rings are a high-performance nickel-chromium alloy known for its excellent high-temperature strength, oxidation resistance (up to 2200°F/1200°C), and carburization resistance. Its typical composition is approximately 58-63% nickel, 21-25% chromium, and 1-1.7% aluminum, with the main applicable standard being ASTM B168/ASME SB168 for flat products. This alloy provides high mechanical strength for components in high-temperature and corrosive environments, such as furnaces and chemical processing equipment.

What are the characteristics of Inconel 601 alloy?

A prominent feature of INCONEL 601 alloy is its excellent resistance to high-temperature oxidation. The alloy also possesses good resistance to aqueous corrosion, high mechanical strength, and is easy to form, machine, and weld.

Inconel 601 Alloy
 

Inconel 601 Ring Specification

 

Nickel Alloy 601 Forged Rings Standards

Inconel 601
UNS N06601
WNR 2.4851

 

Inconel 601 Ring Size

Outer diameter: 145 to 3000 mm
Thickness: 300 mm
End face height: up to 49 inches
Ring weight: 60,000 pounds

 

Forging Method

Die forging/Upset forging
Open die forging/Closed die forging
Cold forging/Hot forging
Impression die forging

 

Packaging

Wooden crates
Plastic packaging
Cardboard boxes

 

Inconel 601 Plate Cut Rings Finish

Forged black
Precision machining

 

Inconel Alloy 601 Socket Ring Testing

Heat treatment
Non-destructive testing/Material composition analysis
Ultrasonic testing
Liquid penetrant testing
Quality assurance

 

Nickel Alloy 601 Forged Rings Size Chart

Ring Diameter (inches) Thickness (inches)
5.25 0.75
6.75 1.25
8.10 0.90
9.50 1.00
10.25 1.50

 

UNS N06601 Rolled Rings Weight Chart

Ring Diameter (inches) Thickness (inches) Weight (lbs) Weight (kg)
3.00 0.50 2.50 1.14
4.00 0.75 5.50 2.49
5.00 1.00 9.00 4.08
6.00 1.25 13.50 6.12
8.00 1.50 20.00 9.07

 

WNR 2.4851 Seal Rings Temprature Rating

Temperature Rating (°F) Temperature Rating (°C) Environment
Up to 1,800 Up to 982 Oxidizing Environments
Higher than 1,800 Higher than 982 Non-Oxidizing Atmospheres
1,800 – 2,000 982 – 1,093 Solution Annealing

 

Types of Inconel 601 Rings

 

Nickel Alloy 601 Forged Rings

Nickel Alloy 601 Forged Rings

UNS N06601 Rolled Rings

UNS N06601 Rolled Rings

WNR 2.4851 Seal Rings

WNR 2.4851 Seal Rings

Ferrochronin 601 Plate Cut Rings

Ferrochronin 601 Plate Cut Rings

Inconel Alloy 601 Socket Ring

Inconel Alloy 601 Socket Ring

Pyromet 601 Hot Forged Rings

Pyromet 601 Hot Forged Rings

Inconel 601 Seamless Rolled Ring

Inconel 601 Seamless Rolled Ring

Custom Nicrofer 601 Ring

Custom Nicrofer 601 Ring

Inconel 601 vs 600

Property Inconel 601 Inconel 600
Chemical Composition Ni: 58-63%, Cr: 21-25%, Fe: 5-10%, Al: 1-1.5%, Ti: 3-4.5% Ni: 72-78%, Cr: 14-17%, Fe: 6-10%
Oxidation Resistance Excellent at high temperatures up to 2200°F (1200°C) Good but lower than 601, up to 2000°F (1093°C)
High-Temperature Strength Good Good
Applications Aerospace, heat treatment, chemical processing Chemical processing, heat exchangers, nuclear reactors
Formability Good Excellent
Corrosion Resistance Good Good

 

Equivalent standards for Ferrochronin 601 sheet metal cutting rings

Standard Equivalent
UNS N06601
WNR 2.4851
AMS 5540
DIN 2.4851
BS 3076

 

Chemical Composition of Inconel Alloy 601 Socket Ring

Element Content (%)
Carbon (C) ≤ 0.10
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.50
Iron (Fe) 5.0 – 10.0
Chromium (Cr) 21.0 – 25.0
Nickel (Ni) 58.0 – 63.0

 

Pyromet 601 Hot Forged Rings Mechanical Properties

Property Value Units
Tensile Strength 110,000 psi
Yield Strength 70,000 psi
Elongation 30 %
Modulus of Elasticity 29 ×106 psi
Hardness 225 HB
Fatigue Strength 50,000 psi

 

Physical Properties of Inconel 601 Seamless Rolled Ring

Property Value Units
Density 8.47 g/cm³
Melting Point 2,350 °F
Melting Point 1,288 °C
Thermal Conductivity 10.6 W/m·K
Specific Heat 0.12 BTU/lb·°F
Coefficient of Thermal Expansion 6.9 µm/m·°C

 

Inconel 601 vs 625

Property Inconel 601 Inconel 625
Nickel (Ni) Content (%) 58-63 58-68
Chromium (Cr) Content (%) 21-25 20-23
Iron (Fe) Content (%) 5-10 5
Tensile Strength (ksi) 80-110 100-130
Yield Strength (ksi) 30-55 70-100
Oxidation Resistance (°F) Up to 2200 Up to 2000
Temperature Range (°F) -321 to 2200 -423 to 2000

 

Inconel 601 ring-shaped parts: Delivery location and shipping time

Inconel 601 ring-shaped parts supplier (conforming to UNS N06601 standard), available for immediate shipment.

Changes in Price
Extra 5 %
Export to Shipping Time in Days
Norway 45
Germany 21
France 28
Italy 28
Uk 30
Spain 30
Ukraine 60
Netherland 30
Belgium 40
Greece 45
Czech Republic 45
Portugal 45
Hungary 45
Albania 45

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

Gnee Steel
 
 

About Gnee Steel

Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry