Nov 09, 2025 Leave a message

ASTM B670 Inconel 718 pickled alloy tubing

 
our casey
 

Gnee Steel

 

ASTM B670 Inconel 718 pickled alloy tubing

ASTM B670 Inconel 718 is a precipitation-hardening nickel-chromium alloy widely used due to its high strength, corrosion resistance, and excellent high and low temperature performance. "Pickling" refers to a surface treatment performed after heat treatment to remove oxide scale. This material is suitable for applications requiring superior mechanical properties under extreme conditions, such as aerospace, gas turbines, and cryogenic technology.

ASTM B670 Inconel 718 pickled alloy tubing

Gnee Steel

 

What are the three main characteristics of Inconel 718?

Inconel 718 is a precipitation-hardening nickel-based alloy designed to exhibit extremely high yield strength, tensile strength, and creep rupture strength at temperatures up to 1300°F.

Inconel 718

Spec Chart of Inconel 718 Pipe

ASTM Specification ASTM B670 / ASME SB670
Standard ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB
Inconel 718 Seamless Pipe Size 4 to 219mm W. T.: 0.5 to 20mm
Inconel alloy 718 Welded Pipe Size 5.0 - 1219.2 mm
Nickel Alloy 718 EFW Pipe size 5.0 - 1219.2 mm
Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
Inconel 718 din 2.4668 Pipe Schedule SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Inconel 718 Pipe Length Single Random, Double Random, Standard & Cut length Pipe
Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc
Form Inconel 718 Pipe are available in form of Round, Square, Hollow, Rectangular, Hydraulic, Coiled, Straight Pipes, "U" Shape, Pan Cake Coils etc.
Type of 718 Inconel Pipe Seamless / ERW/ EFW / Welded / Fabricated / CDW / DOM / CEW Inconel 718 Pipe
Inconel 718 Pipe End Plain End, Beveled End, Treaded Pipe, Screwed ends

 

Mechanical Properties Chart of Inconel 718 Pipe

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
718 8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

 

ASTM B670 UNS N07718 Pipe Chemical Composition Table

Grade C Mn Si Fe S Cr Al Ni
718 min. – – – bal – 17.0 0.2 50.0
max. 0.08 0.35 0.35 bal 0.01 21.0 0.8 55.0

 

Alloy 718 Tube Physical Properties

 

Solution Treated

Solution Treated and Aged

Density

0.296 lb/in3 (8.192 g/cm3)

0.297 lb/in3 (8.22 g/cm3)

Specific Gravity

8.19

8.22

Melting Range

2500-2600°F

1370-1430°C

 

Advantages of Acid Pickling Surface Treatment

Surface Treatment: "Acid pickling" refers to a chemical surface treatment method that typically uses an acid bath to remove surface oxide scale.

Improved Surface Quality: This process yields a clean, oxide-scale-free surface, which is crucial for many high-performance applications with extremely high surface integrity requirements.

 

Why Choose Gnee Nickel Alloy (Supplier Example)?

✅ Large stock of Inconel series alloy tubes/bars/plates/fittings available for fast shipping.

✅ Factory direct sales, highly competitive prices, excellent value for money.

✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical property certificate.

✅ Value-added services: slitting, cutting, polishing, surface treatment.

✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 and Inconel 725, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness 0.1 to 100 mm; width 10-2500 mm); strips; alloy round bars (diameter 3-800 mm); flat bars (thickness 2-100 mm; width 10-500 mm); hexagonal bars (size 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide customers with 600/725 alloys, whose products meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600 and Inconel 725, pipes, tubes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel
ASTM B670 Inconel 718 pickled alloy tubing
ASTM B670 Inconel 718 pickled alloy tubing
ASTM B670 Inconel 718 tubing
ASTM B670 Inconel 718 tubing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry