ASTM B167 Inconel 600 Seamless Nickel Alloy Industrial Corrosion-Resistant Pipe

 
ASTM B167 Inconel 600 Seamless Nickel Alloy Industrial Corrosion-Resistant Pipe

ASTM B167 Inconel 600 Seamless Nickel Alloy Industrial Corrosion-Resistant Pipe

 

ASTM B167 Inconel 600 seamless steel pipe is a nickel-chromium alloy steel pipe renowned for its high strength, excellent corrosion resistance, and high-temperature performance, making it suitable for harsh industrial environments. Its key characteristics include resistance to chloride ion stress corrosion cracking, high-temperature oxidation, and corrosion from corrosive chemicals such as chlorine and hydrogen chloride. This steel pipe is widely used in demanding applications in the chemical, petrochemical, nuclear, and heat treatment industries.

What temperatures can Inconel 600 withstand?

 

The hot working temperature range for Inconel 600 alloy is 1600 – 2250°F (870 – 1230°C). Heavy-duty working requires temperatures between 1900 – 2250°F (1040 – 1230°C), while light-duty working can be performed at temperatures as low as 1600°F (870°C).

Inconel 600

ASTM B167 UNS N06600 Inconel 600 Pipe Specifications

Specifications ASTM B 167 ASME SB 167 / ASTM B 517 ASME SB 517, ASTM B 829 ASME SB 829 / ASTM b167 n06600 cl.h.f, ASTM b167 alloy n06600
Common Standards SAE/ AMS 5580, N-253, ISO 6207, MIL-DTL-23227, and N-576, ASTM B 751/ ASME SB 751, DIN 17751, ASTM B 517/ ASME SB 517, N-20, ASTM B 167/ ASME SB 167, ASTM B 163/ ASME SB 163, ASME Code Cases 1827, ASTM B 516/ ASME SB 516, ASTM B 829/ASME SB 829, ASTM B 775/ ASME SB 775
SMLS B167 UNS N06600 4 to 219mm W. T.: 0.5 to 20mm
Welded / ERW 5.0 mm – 1219.2 mm
Pipes Sch. Inconel 600 ASTM B167 SCH5, SCH10, SCH40, STD, SCH80, SCH160
Different Types Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes
Forms Include Round, Hydraulic Etc
Lengths available Single Random, Double Random & Cut Length.
Pipe End Finish BBE, BSE, BE, BLE, BOE, TOE, BOE, POE, TBE, PBE

 

600 Inconel Pipe Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

 

Inconel 600 Seamless Pipe Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

 

Equivalent Material of Alloy 600 Pipe

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 600 2.4816 N06600 NCF 600 NA 13 28-2,5-1,5 NC15FE11M NiCr15Fe

 

Why Choose Gnee Nickel Alloy (Supplier Example)?

✅ Large stock of Inconel series alloy tubes/bars/plates/fittings available for fast shipping.

✅ Factory direct sales, highly competitive prices, excellent value for money.

✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical property certificate.

✅ Value-added services: slitting, cutting, polishing, surface treatment.

✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 and Inconel 725, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness 0.1 to 100 mm; width 10-2500 mm); strips; alloy round bars (diameter 3-800 mm); flat bars (thickness 2-100 mm; width 10-500 mm); hexagonal bars (size 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide customers with 600/725 alloys, whose products meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600 and Inconel 725, pipes, tubes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel
ASTM B167 Inconel 600 Seamless Nickel Alloy Industrial Corrosion-Resistant Pipe
ASTM B167 Inconel 600 Seamless Nickel Alloy Industrial Corrosion-Resistant Pipe
ASTM B167 Inconel 600 Seamless Nickel Alloy Pipe
ASTM B167 Inconel 600 Seamless Nickel Alloy Pipe

Send Inquiry

whatsapp

Phone

E-mail

Inquiry