ASTM B166 Inconel 600 Round Bar for Heat Exchangers

Introduction

ASTM B166 UNS N06600 is a nickel-chromium-iron alloy round bar recognized for excellent high-temperature oxidation resistance and immunity to chloride-induced stress corrosion cracking. The combination of high strength and good mechanical properties at both room and elevated temperature makes it a common choice for heat exchangers, furnace components, and chemical processing equipment. The specification is widely referenced internationally through the ASME SB166 counterpart for pressure equipment applications.

Specification Scope

ASTM B166 covers nickel-chromium-iron alloy bar, rod, and wire products including UNS N06600, N06601, N06603, N06690, N06693, N06025, N06045, and N06696, as well as the nickel-chromium-cobalt-molybdenum alloy UNS N06617. Product forms include hot-worked and cold-worked rod, and bar in rectangular, hexagonal, square, and round solid sections, supplied in the annealed condition unless otherwise agreed. Sizes cover rectangular and square sections up to 254 mm in width with thickness of 3.2 mm and over, in straight lengths, with length supplied as specific or random as ordered.

Chemical Composition

The typical composition limits for UNS N06600 under ASTM B166 are nickel 72.00 percent minimum, chromium 14.00 to 17.00 percent, iron 6.00 to 10.00 percent, copper 0.50 percent maximum, manganese 1.00 percent maximum, carbon 0.15 percent maximum, silicon 0.50 percent maximum, and sulfur 0.015 percent maximum. The high nickel content provides resistance to chloride stress corrosion cracking and caustic media, while chromium contributes oxidation resistance at elevated temperatures.

Mechanical and High-Temperature Properties

N06600 bars exhibit good strength and toughness at both room and high temperatures, high resistance to carburizing and nitriding, and do not become brittle after prolonged high-temperature exposure. The alloy withstands high pressure and high temperature without deformation, and performs well in environments where traditional stainless steel is prone to oxidation, such as heat treatment and petrochemical service. Exact minimum values required for procurement are defined in the specification and depend on product form and size, so the applicable standard and mill test certificate should always be consulted.

Corrosion Resistance

The alloy offers outstanding resistance to a wide range of chemicals, including chloride stress corrosion cracking, and performs reliably in oxidizing and alkaline environments. It resists dry chlorine up to about 538 °C and oxidation up to about 1093 °C, which makes it suitable for heat exchangers, caustic soda production equipment, and furnace components where both temperature and corrosive media are present.

Typical Applications

Common applications include heat exchangers, chemical and food processing equipment, furnace components, nuclear engineering parts, pressure vessels, gas and power plant components, and general manufacturing. For heat exchanger service, the round bar form is frequently machined into tube sheets, baffles, flanges, and structural supports where high-temperature strength and corrosion resistance must be combined.

Fabrication Notes

Inconel 600 is readily hot and cold worked and can be welded by common processes with matching filler metal. Hot working is typically carried out in the range of 870 to 1230 °C, with heavy working between 1040 and 1230 °C. Annealing restores corrosion resistance after cold working. When machining, use sharp tools and rigid setups because the alloy tends to work-harden.

FAQ

Q: What standards cover Inconel 600 round bar?

A: ASTM B166 and ASME SB166 are the governing specifications for bar, rod, and wire, covering UNS N06600 and related nickel-chromium-iron alloys. Pipe and tube are covered by ASTM B167, and plate, sheet, and strip by ASTM B168.

Q: Is Inconel 600 bar suitable for heat exchangers?

A: Yes. Its combination of high-temperature strength, oxidation resistance, and immunity to chloride stress corrosion cracking makes it a proven material for heat exchanger components in chemical, petrochemical, and power applications.

Q: How does Inconel 600 compare with Inconel 625?

A: Inconel 625 has higher chromium and molybdenum, giving better overall corrosion resistance and higher mechanical properties, while Inconel 600 offers a more economical solution for high-temperature oxidation and chloride service where maximum strength is not required.

Q: What is the annealed condition?

A: Annealing is a heat treatment that softens the material, restores ductility, and removes the effects of cold work, typically performed at about 980 to 1065 °C followed by rapid cooling, depending on section size.

Q: Can Inconel 600 bar be welded?

A: Yes. Inconel 600 has excellent weldability using standard processes with matching nickel-based filler metal, and is widely fabricated into equipment without special preheat in most cases.

Q: What size ranges are typical for round bars?

A: Industry supply commonly ranges from about 3 mm to 300 mm diameter for round bars, with larger sizes available by special arrangement. Confirm the exact range and tolerance with the supplier against the specification.