ASTM A519 AISI 4130 alloy seamless steel pipe introduction
4130 is a chromium-molybdenum alloy steel pipe model.
Chromium-molybdenum steel alloy steel pipe is a kind of seamless steel pipe, and its performance is much higher than that of ordinary seamless steel pipe. Because this type of steel pipe contains more Cr, its high temperature, low temperature and corrosion resistance are unmatched by other seamless steel pipes. Therefore, alloy pipes are widely used in petroleum, chemical, electric power, boiler and other industries.
What kind of steel pipe is 4130?
4130 corresponds to the domestic grade 30CrMo, and the tensile strength is generally above 700MPa. The welding wire needs to use ER70-G high-strength welding wire, which can be asked when purchasing.


ASTM A519 AISI 4130 alloy seamless steel pipe introduction
Alloy steel pipe grade: AISI 4130
Standard: ASTM A29/A29M-04. ASTM A519
Corresponding domestic brand: 30CrMo
Corresponding Japanese brand: SCM430 (SCM2)
Corresponding German brand: 34CrMo4 (1.7220)
American standard A519 4130 seamless steel pipe for petroleum machinery
American standard AISI4130 seamless steel pipe implementation standard: ASTM A519
American standard ASTM/AISI 4130 alloy steel pipe chemical composition: C: 0.28~0.33 Si: 0.15~0.35 Mn: 0.40~0.60 S≤0.040 P≤0.040 Cr: 0.80~1.10 Mo: 0.15~0.25
American standard AISI 4130 mechanical properties: tensile strength: ≥620MPa, yield strength: ≥415MPa, elongation after fracture: ≥20%, can also be tempered according to customer requirements
American standard AISI4130 alloy steel pipe delivery status: hot rolling or tempering heat treatment
Specifications: 60.3-765*5-120, commonly used diameters: 60.3, 73, 88.9, 101.6, 114.3, 141.3, 168.3, 219.1, 273.1, 323.9, 355.6, 406.4, 457.2, 508, 559, 610, 660, 711, 762. Other sizes can also be customized according to customer requirements.
American standard 4130 seamless steel pipe application areas: mainly used for oil exploration equipment, drilling equipment, mechanical oil production equipment, oil drilling equipment and accessories, oil and gas gathering and transportation complete sets of materials required