Feb 04, 2024 Leave a message

Hot Rolling Clad Heads for Pressure Vessels and Heat Exchangers

Cylindrical shells, nozzles and dished ends are the parts of a pressure vessel that contact the process fluid, so they are frequently made from a corrosion-resistant alloy. A clad head solves the cost problem: the corrosion-resistant layer is bonded to a carbon or low-alloy steel backing, and the backing carries the structural load while the cladding faces the process.

What Is a Hot Rolling Clad Head

A clad head is a formed vessel end built from a clad plate that consists of two or more layers of dissimilar metal. The outer or working layer, called the cladding, is a corrosion-resistant alloy, while the inner layer, called the backing, is usually carbon steel or low-alloy steel. Manufacturers produce clad plate by explosion bonding, roll bonding or hot rolling, and the bonded plate is then cut and formed into the required head shape, such as a 2:1 ellipsoidal, torispherical, hemispherical, conical or flat head.

The Hot Roll Bonding Process

Preparation. The cladding plate and the backing plate are flattened and their mating surfaces are cleaned to remove oxides, grease and dirt, because any contamination left on the interface becomes a bond defect.

Assembly. The two plates are stacked, aligned and fixed together at the edges so that they cannot shift during handling and rolling.

Heating. The pack is heated to a temperature above the recrystallisation temperature of the materials, typically in the range of 1100–1200 °C, chosen so that both metals deform readily without melting or excessive grain growth.

Rolling. The heated pack is passed through a rolling mill. The combination of heat and roll pressure causes the surfaces to deform together and creates a metallurgical bond across the whole interface rather than a mechanical interlock.

Finishing. The bonded plate is rolled to the required total thickness, cooled, cut to the developed head blank, then hot or cold formed to the head profile and trimmed, with the cladding thickness maintained over the crown and knuckle.

Cladding and Backing Material Combinations

Layer Material Specification Reason for selection
Cladding 304L / 316L stainless steel ASTM A240 General corrosion resistance at moderate temperature
Cladding Alloy 800H / UNS N08810 ASTM B409 Oxidation and carburisation resistance in hot process streams
Cladding Alloy 625 / UNS N06625 ASTM B443 Severe oxidising and chloride-bearing service
Cladding Alloy C-276 / UNS N10276 ASTM B575 Reducing acids and mixed corrosive media
Cladding Titanium Grade 2 / UNS R50400 ASTM B265 Seawater and oxidising chloride service
Backing Carbon steel plate ASTM A516 Grade 70 Pressure-retaining strength at moderate temperature
Backing Chromium-molybdenum steel ASTM A387 Higher temperature and hydrogen service

Because the two layers must deform together, the combinations are not freely interchangeable. Titanium, for example, forms brittle phases with steel at bonding temperature, so an interlayer is normally used, and the bonding schedule is developed for each combination rather than taken from a general table.

Advantages of Hot Roll Bonding

Large clad plates can be produced, which makes it possible to form heads and shell courses of sizes that other bonding routes cannot supply in one piece.

The bond is metallurgical and continuous over the bonded area, so heat transfer through the head is not interrupted by an interlayer of air or adhesive.

A wide range of total thicknesses, cladding thicknesses and head profiles can be produced from the same route.

The process needs fewer handling steps than some alternative bonding methods, which keeps the cost of the finished head competitive.

The backing steel can be selected for strength and code compliance while the cladding is selected purely for corrosion resistance, giving an economical combination that a solid alloy head cannot match.

Quality Control, Forming and Applications

Clad plate for pressure equipment is ordered to specifications such as ASTM A263, A264 or A265, which cover stainless steel, chromium-nickel and nickel alloy cladding on steel plate respectively. Those specifications require the bond to be verified by ultrasonic examination, normally to ASTM A578, and to meet a minimum shear strength determined by the applicable specification. After forming, the head is checked for overall dimensions, cladding thickness over crown and knuckle, surface condition of the cladding and freedom from disbonding at the knuckle, where forming strains are highest. Formed head tolerances are governed by the pressure vessel code, for example ASME BPVC Section VIII Division 1.

Typical applications include pressure vessels and heat exchangers in oil and gas production and refining, distillation columns and reactors in the chemical industry, desalination and flue gas desulfurisation equipment, and storage or process vessels in pulp and paper plants. In each case the clad head allows a corrosion-resistant wetted surface with a pressure-retaining steel backing.

Frequently Asked Questions

Q: What is a hot rolling clad head?
It is a formed pressure vessel end made from a clad plate in which a corrosion-resistant alloy layer has been bonded to a carbon or low-alloy steel backing by heating and rolling the two plates together.

Q: How does hot roll bonding differ from explosion bonding?
Explosion bonding joins the plates with a high-velocity impact wave at ambient temperature, while hot roll bonding uses elevated temperature and roll pressure. Roll bonding is well suited to large plates and to combinations that can be co-deformed at temperature.

Q: At what temperature are the plates bonded?
Bonding is carried out above the recrystallisation temperature of the materials, typically around 1100–1200 °C, with the exact schedule set by the cladding and backing combination.

Q: How is the bond quality verified?
The clad plate specification requires ultrasonic examination, normally to ASTM A578, together with shear strength testing of a bonded test piece, and after forming the head is inspected for cladding thickness and disbonding.

Q: Why not make the whole head from the corrosion-resistant alloy?
A solid alloy head of the same pressure rating would be far more expensive and, for large diameters, difficult to obtain. Cladding puts the costly alloy only where it contacts the process, while the steel backing provides the strength.

Q: Can cladding be damaged during forming?
Forming strains are highest at the knuckle, so the bonding schedule, cladding thickness and forming temperature are selected to keep the cladding intact. Ultrasonic and visual inspection after forming is used to confirm that the bond and the cladding surface remain sound.