Advantages and applications of Hastelloy C276 round bars

Advantages and applications of Hastelloy C276 round bars
Hastelloy C276 round bars possess excellent corrosion resistance (pitting and crack resistance), superior high-temperature mechanical strength, and good machinability, making them an ideal choice for harsh environments such as chemical processing, oil and gas, pulp and paper, flue gas desulfurization (FGD), and waste treatment. They are used in heat exchangers, reactors, pumps, and pipelines to ensure service life and prevent failures when other metals fail.
Is Hastelloy C276 resistant to sulfuric acid corrosion?
C-276 alloy exhibits excellent resistance to sulfuric acid, hydrochloric acid, formic acid, acetic acid, chlorides, solvents, wet chloride gases, hypochlorites, and chlorine solutions. It also demonstrates excellent resistance to phosphoric acid corrosion at all temperatures below its boiling point and in phosphoric acid solutions with a concentration below 65%.

What is Hastelloy C276 Round Bar?
Hastelloy C276 round bar possesses excellent corrosion resistance and high-temperature strength. It is a nickel-molybdenum-chromium alloy with added tungsten, designed to provide superior corrosion resistance in a variety of harsh environments. Hastelloy C276 round bar is widely used in the manufacture of components in chemical, pollution control, pulp and paper, nuclear fuel reprocessing, acid production, and waste treatment industries. Hastelloy C276 round bar exhibits excellent resistance to localized corrosion, such as pitting and stress cracking. It can be machined into various shapes, including hexagonal, round, flat, square, and rectangular. This product features high tensile strength, excellent weldability and formability, a low coefficient of thermal expansion, and good toughness.
Hastelloy C276 Alloy Bar Chemical Composition
|
Element |
Percentage (%) |
|
Nickel (Ni) |
Balance |
|
Molybdenum (Mo) |
15.0 – 17.0 |
|
Chromium (Cr) |
14.5 – 16.5 |
|
Iron (Fe) |
4.0 – 7.0 |
|
Tungsten (W) |
3.0 – 4.5 |
|
Cobalt (Co) |
≤ 2.5 |
|
Manganese (Mn) |
≤ 1.0 |
|
Vanadium (V) |
≤ 0.35 |
|
Silicon (Si) |
≤ 0.08 |
|
Carbon (C) |
≤ 0.01 |
|
Sulfur (S) |
≤ 0.03 |
|
Phosphorus (P) |
≤ 0.04 |
Mechanical Properties of Hastelloy C276 Round Bar
|
Property |
Value |
|
Tensile Strength |
690 MPa (min) |
|
Yield Strength (0.2% offset) |
283 MPa (min) |
|
Elongation |
40% |
|
Hardness (Rockwell B) |
≤ 100 |
|
Density |
8.89 g/cm³ |
|
Melting Point |
1325 – 1370°C |
Key Properties of Hastelloy C276 Round Bars
Corrosion Resistance: Resistant to pitting corrosion, stress corrosion, and acid corrosion (hydrochloric acid, sulfuric acid, nitric acid, phosphoric acid)
Weldability: Easily weldable using GTAW, SMAW, and MIG welding without post-weld heat treatment.
High Temperature Resistance: Withstands temperatures up to 1000°C in both oxidizing and reducing environments.
Formability: Suitable for machining, forging, and cold/hot forming; can be produced into various custom shapes.
Industrial Applications of Hastelloy C276 Round Bars
|
Industry |
Applications |
|
Chemical Processing |
Reactors, scrubbers, heat exchangers, mixers |
|
Oil & Gas |
Subsea valves, manifolds, risers, drill collars |
|
Pharmaceuticals |
Acidic processing tanks, sterilization components |
|
Pulp & Paper |
Bleaching towers, digesters, chemical recovery systems |
|
Waste Treatment |
Incinerators, evaporators, waste processing systems |
|
Marine |
Pump shafts, propeller shafts, deep-sea components |
Advantages of Hastelloy C276 Round Bars
Hastelloy round bars exhibit the characteristics of nickel alloys in a variety of applications. It is a nickel-chromium superalloy rich in molybdenum, with controlled tungsten and iron content and extremely low carbon content. Due to the low carbon content, carbide deposition is limited during heat treatment and welding.
This means that the metal maintains excellent resistance to pitting and crevice corrosion in welding systems. Compared to other materials, Hastelloy C276 round bars may experience a decrease in weld strength after welding heating, leading to a decline in its corrosion resistance. This material possesses extremely strong corrosion resistance, including resistance to stress corrosion cracking and crevice corrosion.
Hastelloy C-276 is a globally leading corrosion-resistant nickel-chromium-molybdenum alloy. Under various chemical conditions, including high-temperature contaminated mineral acids, solvents, chlorine gas and chlorine-contaminated environments (including physical and chemical contamination), hypochlorite and chlorine dioxide solutions, dry chlorine gas, formic acid and acetic acid, acetic anhydride, seawater, and brine solutions, C276 alloy exhibits excellent corrosion resistance.
In the weld state, C276 alloy exhibits minimal grain boundary precipitate formation in the weld heat-affected zone, making it suitable for most chemical applications. It possesses exceptional resistance to pitting and stress corrosion cracking. It is no surprise that Hastelloy C276 round bars are widely used in numerous commercial sectors due to their superior durability.
The high molybdenum content further enhances its resistance to pitting and stress corrosion cracking. Wastewater treatment systems utilize this metal when other metals fail to maintain their performance under harsh conditions.
Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners
📦 Packaging and Shipping
All stainless steel products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express

About Gnee Steel
Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.
Square Meters Built
Enterprise Employees
Years Experience
Partner countries