Inconel 718 Round Bar

About Inconel 718 Round Bar
Inconel 718 round bar is a high-strength, corrosion-resistant nickel-chromium alloy known for its excellent high-temperature performance and ease of machining and welding. It is widely used in aerospace, oil and gas, and other demanding applications.
What is the composition of Inconel 718 round bar?
Inconel 718 Round Bar is a nickel chromium alloy bar that has up to 55% nickel in the composition. The content includes 17% chromium, 4.9% niobium, 6.6% iron minimum and aluminum, boron, carbon, cobalt, copper, manganese, phosphorus, lead, sulfur and silicon.

Mechanical Strength Table Chart Alloy 718 Round Bar
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 718 | 8.14 g/cm3 | 1400 °C (2550 °F) | Psi – 80,000 , MPa – 550 | Psi – 32,000 , MPa – 220 | 30 % |
Chemical Compatibility Chart of Inconel 718 Round Bar
| Grade | C | Mn | Si | Fe | S | Cr | Al | Ni | |
| 718 | min. | – | – | – | bal | – | 17.0 | 0.2 | 50.0 |
| max. | 0.08 | 0.35 | 0.35 | bal | 0.01 | 21.0 | 0.8 | 55.0 | |
Hardness of Inconel Alloy 718 Round Bar
| 0.2% Proof Stress | Tensile Strength | Elongation | Reduction of area | Hardness |
|---|---|---|---|---|
| MPA | MPA | % | % | HRC |
| Min | Min | Min | Min | Min |
| 827 | 1034 | 17 | 25 | 40 |
Size Chart of Nickel 718 Bar
| Size & Dimensions of inconel 718 round bar | |||||||
|---|---|---|---|---|---|---|---|
| Metric | US Bar | ASTM/ Canadian | Japanese | ||||
| Bar Size | Diam. (mm) | Bar Size | Diam. (Inch) | Bar Size | Diam. (mm2) | Bar Size | Diam. (mm) |
| 5 | 5 | #2 | 0.250 | 10M | 100 | 6 | 6 |
| 5.5 | 5.5 | #3 | 0.375 | 15M | 200 | 10 | 10 |
| 6 | 6 | #4 | 0.500 | 20M | 300 | 13 | 13 |
| 7 | 7 | #5 | 0.718 | 25M | 500 | 16 | 16 |
| 8 | 8 | #6 | 0.750 | 30M | 700 | 19 | 19 |
| 9 | 9 | #7 | 0.875 | 35M | 1000 | 22 | 22 |
| 10 | 10 | #8 | 1.000 | 45M | 1500 | 25 | 25 |
| 11 | 11 | #9 | 1.125 | 55M | 2500 | 29 | 29 |
| 12 | 12 | #10 | 1.250 | 32 | 32 | ||
| 14 | 14 | #11 | 1.375 | 35 | 35 | ||
| 16 | 16 | #12 | 1.500 | 38 | 38 | ||

Gnee Steel specializes in the production of various nickel-based alloys. Gnee Steel's product packaging includes steel strapping: Pipes with an outer diameter of 3 inches or less are typically strapped together with polypropylene film to prevent rust during sea transportation, and then secured with steel strapping. Wooden boxes/crates: Pipes are typically packaged in wooden boxes or crates to protect them during transportation, especially those that are longer or have larger diameters. Seaworthy export packaging: Suppliers typically use standard seaworthy export packaging methods, which may include a variety of materials and techniques to protect the pipes during transportation. Tarpaulin packaging: This prevents rain, seawater, and other external factors from penetrating the export wooden crates during transportation. Gnee Steel specializes in the production and sale of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy industries, and we can provide customized alloy material solutions based on customer needs. For alloy material pricing inquiries or customized alloy material solutions, please contact us for a quote at ss@gneesteel.com.