Inconel X750 Round Bar
video

Inconel X750 Round Bar

Similar grades: GH4145 (China), NiCr15Fe7TiAl (Germany), NC15FeTNbA (France), NCF750 (Japan)
Certification: ISO9001:2015
Alloy category: corrosion-resistant alloy
Substrate shape: axial wire/strip/straight bar
Alloy series: nickel-chromium alloy
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel x750 round bar in China. If you're going to wholesale high quality inconel x750 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel x-750 alloy bar (UNS No. 7750/W.NR.2.4669) is a nickel-chromium based precipitation hardening high temperature alloy with good corrosion resistance and oxidation resistance below 980, high strength below 800, good creep resistance below 700, and good relaxation resistance below 540.

 

Inconel X-750 casting process

The alloy is remelted by electric arc furnace plus vacuum material, vacuum induction plus electroslag, electroslag plus vacuum material or vacuum induction plus vacuum material.

 

Inconel X-750 Cold Rolled Steel Bar Applications
This alloy has been used in the manufacture of aircraft, components and bolts that are highly corrosive and require high or low stress on a flat waveform with high strength and corrosion resistance.

 

Specifications of Inconel X-750 Alloy Bars
X-750 Alloy Bars Chemical Composition
Weight % Ni +(Co) Cr Fe Ti Al Nb + (Ta) Mn Si S Cu C Co
X-750
UNS N07750
70 min 14-17 5-9 2.25-2.75 0.40-1.0 0.70-1.2 1 max 0.50 max 0.01 max 0.50 max 0.08 max 1 max
UNS N07752 is available in billets for forging. UNS N0772 has limits of 0.05% on both Carbon and Cobalt
 

Inconel X-750 Alloy Round Bars Typical Mechanical Properties

Material Size Ultimate
Tensile Strength ksi
Yield Strength (0.2% Offset) Ksi Elongation in 4D(%) % Reduction of Area
Alloy X-750 Bar Under 4.0" 165.0 105 20 25
Alloy X-750 Bar 4.0 " and over 160 100 15 17
Properties as described in AMS 5667 which requires that material following 1625°F/24 hrs, AC-Equalising + precipitation treatment have the following minimum room temperature properties. Hardness will lie in the range of 302-363 BHN
Inconel x-750 Round Bar

Inconel x-750 Round Bar

Why choosing GNEE

GNEE has five finishing rolling lines and two hot rolling lines. In addition, we also adopt more advanced automatic width control system (AWC), automatic thickness control system (AGC), bending roll system, work roll groove roll system and other effective measures to ensure product quality.

In addition, GNEE also provides InconelX-750 Square Bar, InconelX-750 hot finished hexagon Rods, Inconel X-750 Cold Drawn Flat Bar.

please contact us for a quote! ss@gneesteel.com

Industry-leading inconel alloy production testing

Industry-Leading Inconel Alloy

inconel X-750 suppliers

Inconel X-750 Suppliers

Nickel Alloy X-750 PACKAGING AND SHIPPING

​​Nickel Alloy X-750

FAQ

1.Q.How can I trust you?
A. We think honesty is the core of our company, you can come to know it personally so that you can check our credit.

2.Q.Can your products be customized?
A.Yes, we can produce and process according to your requirements.

3.Q. Do you have a quality control system?
A.Yes, we have our own quality control laboratory.

Hot Tags: inconel x750 round bar, China inconel x750 round bar suppliers, Inconel 713C 625 Pipe, inconel alloy exhaust system parts, inconel alloy metal tube, lnconel 718 alloy, inconel alloy combustion chamber parts, inconel alloy capacitor parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry