200 660 Pipe
video

200 660 Pipe

nickel 200 is a nickel alloy. Nickel 200 alloy has the following properties: Nickel200 is pure commercial pure nickel with excellent mechanical properties and corrosion resistance
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 200 660 pipe in China. If you're going to wholesale high quality 200 660 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Pipe Products Application

inconel 200 660 Pipe video

Jet engine components

Fasteners

Springs

Bolts

Flanges

Blades

Afterburners

Automotive applications

Offshore oil and gas applications

Moderate corrosion applications in aqueous solutions

Non-magnetic cryogenic equipment

inconel Material Specification

 

The chemical composition of super alloy A-286 is outlined in the following table.

Element Content (%)
Iron, Fe 54
Nickel, Ni 25.5
Chromium, Cr 14.8
Titanium, Ti 2.13
Molybdenum, Mo 1.30
Manganese, Mn 1.0
Silicon, Si 0.50
Vanadium, V 0.30
Aluminum, Al 0.18
Carbon, C 0.040
Phosphorous, P 0.020
Sulfur, S 0.015
Boron, B 0.0060

200 660 Pipe

alloy 200 660 Pipe suppliers200 660 alloy ss Pipe dealer

nickel 200 is a nickel alloy. Nickel 200 alloy has the following properties: Nickel200 is pure commercial pure nickel with excellent mechanical properties and corrosion resistance, high thermal and electrical conductivity, low gas content and low vapor pressure.
660 stainless steel is a Fe-25Ni-15Cr-based high-temperature alloy, which is comprehensively strengthened by adding molybdenum (Mo), titanium (Ti), aluminum (Al), vanadium (V) and trace amounts of boron (B). It has high yield strength, durability and creep strength below 650℃, and has good processing plasticity and satisfactory welding performance. It is suitable for manufacturing high-temperature load-bearing parts of aeroengines that operate below 650°C for a long time, such as vortex, press disk, rotor blades and fasteners.

Customer Case

customer visit

200 660 inconel seamless Pipe price

200 660 stainless steel Pipe for sale

FAQ

 

 

 

Q: What is your delivery time?
A: Our delivery time is about one week, based on the number of customers.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: Can I get a sample before ordering?
A: Yes, of course. Usually our samples are free. We can produce according to your samples or technical drawings.

Q: About the product price of 200 660 Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: 200 660 pipe, China 200 660 pipe suppliers, lnconel 601 round bar, inconel alloy pump parts, Inconel 617 Super Stainless Pipe, inconel alloy reaction injection molding process, inconel alloy socket parts, inconel alloy radar system parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry