Inconel Alloy X-750 Seamless Pipe
video

Inconel Alloy X-750 Seamless Pipe

Available Formats
GNEE Group offers Nickel Alloy Inconel X-750in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy x-750 seamless pipe in China. If you're going to wholesale high quality inconel alloy x-750 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy X-750 Seamless Pipe introduce

Alloy X-750 Seamless Pipe

Inconel Alloy seamless pipeInconel Alloy X-750 pipeInconel Alloy X-750 ss pipe

Inconel X-750 ss pipe is a high-strength, precipitation-hardened nickel-chromium alloy designed for applications requiring excellent mechanical properties at elevated temperatures. Unlike Inconel 625, which relies on solid solution strengthening, Alloy X-750 (UNS N07750) gains strength through heat treatment (aging), making it ideal for high-stress, high-temperature environments.

Inconel X-750 pipe is widely used for its corrosion and oxidation resistance, as well as its high strength at temperatures up to 1300°F. While much of the effect of precipitation hardening disappears as temperatures exceed 1300°F, heat-treated material still has useful strength up to 1800°F.

Specifications of inconel X750 pipe:
Size 1 / 8″ NB – 12″ NB
Specifications ASTM B751, ASME SB751, AMS 5582, AMS 5583
Standard ASTM, ASME
Surface Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
Techniques Hot-rolled, cold-drawn
Length 5.8M,6M,12M & Required Length
Outer Diameter 6.00 mm OD up to 914.4 mm OD
Thickness 0.6 mm to 12.7 mm
Schedule SCH. 5, 10, 20, 30, 40, 60, 80, 100, 120, 140, 160, XXS
Types Seamless or Welded Pipes
Form Round, Square, Rectangle, Hydraulic, Honed Tubes
End Plain End, Beveled End, Treaded
Application Oil Tube, Gas Tube, Fluid Tube, Boiler and Heatexchanger

Inconel X750 Pipes & Tubing Chemical Composition

Grade C Mn Si S Cu Cr Ni
Inconel X750 .08 max 1.00 max .50 max .01 max 0.50 max 14.0 – 17.0 70.0 min

Alloy X750 Pipe and Tubes Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel X750 8.28 g/cm3 1430°C 1267 MPa 868 MPa 25 %

GNEE Group Factory Environment

Inconel Alloy Seamless Pipe

Inconel Alloy X-750 Seamless Pipe

GNEE Group Product Packaging 

Inconel Seamless Pipe

Inconel Alloy X-750 Seamless Pipe

FAQ

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.