Inconel Alloy 783 Seamless Pipe
video

Inconel Alloy 783 Seamless Pipe

Super alloys are also known as high performance alloys specially designed to cater to environments with very high temperature of above 540°C (1000°F) where deformation resistance and high surface stability are essential. Super alloy INCONEL 783 is a nickel-cobalt-iron alloy with chromium, aluminum, and niobium additions. It has oxidation-resistance, low coefficient of thermal expansion. This alloy can be strengthened by a precipitation-hardening heat treatment. The presence of aluminum provides this alloy excellent resistance to oxidation at high temperature.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 783 seamless pipe in China. If you're going to wholesale high quality inconel alloy 783 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 783 is a high-performance nickel-based superalloy that is designed for use in high-temperature applications, such as those found in the aerospace and power generation industries. It exhibits excellent strength and creep resistance at elevated temperatures, making it suitable for use in components like gas turbine engines, heat exchangers, and nuclear reactors.

When it comes to seamless pipe made from Inconel Alloy 783, the material retains its superior mechanical and corrosion-resistant properties. Seamless pipes are fabricated through a process that involves heating a solid metal billet and then piercing it with a mandrel to create a hole. The billet is then drawn or extruded over a form to produce a pipe with no weld seams. This manufacturing method ensures greater integrity and consistency of the pipe wall, which is critical in high-pressure and high-temperature applications.

The chemical composition of INCONEL 783 is outlined in the following table.

Element Content (%)
Nickel, Ni 26-30
Iron, Fe 24-27
Aluminum, Al 5-6
Chromium, Cr 2.5-3.5
Niobium, Nb 2.5-3.5
Copper, Cu 0.50 max
Manganese, Mn 0.50 max
Silicon, Si 0.50 max
Titanium, Ti 0.10-0.40
Carbon, C 0.03 max
Boron, B 0.003-0.012
Phosphorus, P 0.015 max
Sulfur, S 0.005 max
Cobalt, Co Balance

Physical Properties

The physical properties of INCONEL 783 are tabulated below.

Properties Metric Imperial
Density 7.81 g/cm3 0.282 lb/in3
Melting point 1336-1407 °C 2437-2565 °F

 

Inconel Alloy 783 seamless pipeInconel Alloy 783 seamless pipeInconel Alloy 783 seamless pipe

Hot Tags: inconel alloy 783 seamless pipe, China inconel alloy 783 seamless pipe suppliers, high nickel corrosion alloys, inconel tube, inconel alloy transceiver parts, inconel alloy valve parts, inconel alloy control system parts, alloy seamless tubing