Inconel Alloy 603XL Tube
video

Inconel Alloy 603XL Tube

INCONEL alloy 603XL is a nickel-chromium alloy with the addition of molybdenum, silicon, and rare earth elements. The key characteristics of this alloy are its resistance to elevated temperature oxidation and nitridation.INCONEL alloy 603XL is known to be resistant to oxide spalling thus making this alloy very useful in areas where oxide contamination cannot be tolerated such as electronics, ceramics, glass, and tableware industries.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 603xl tube in China. If you're going to wholesale high quality inconel alloy 603xl tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Inconel Alloy 603XL is a nickel-chromium alloy specifically designed for high corrosion resistance in various severe environments. This alloy is known for its excellent resistance to stress corrosion cracking (SCC) and intergranular attack, making it particularly suitable for applications involving aggressive chemicals or high temperatures.

Physical Properties

Density g/cm3 8.54
lb/in.3 0.308
Melting Range °F 2516 - 2552
°C 1380 - 1400

 

Mechanical Properties

The following table shows mechanical properties of INCONEL alloy 603XL alloy.

Properties Metric Imperial
Poisson's ratio 0.33 0.33
Elastic modulus 218.6 GPa 31.8 psi
Shear modulus 81.9 GPa 11.9 psi

Thermal Properties

The thermal properties of INCONEL alloy 603XL are tabulated below.

Properties Metric Imperial
Thermal expansion co-efficient (@100°C/400°F) 12.87 µm/m°C 7.46 µin/in°F
Thermal conductivity(@23°C/200°F) 11 W/mK 74.453 BTU in/hr.ft².°F

 

Inconel Alloy 603XL TubeInconel Alloy 603XL TubeInconel Alloy 603XL Tube

Hot Tags: inconel alloy 603xl tube, China inconel alloy 603xl tube suppliers, inconel alloy reaction injection molding process, inconel alloy piston parts, inconel seamless piping, inconel alloy seamless piping, inconel alloy valve parts, inconel alloy intake system parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry