Inconel Alloy 601 UNS N06601 elbow fitting
Welded Fittings: 1/2" - 48"
Standards: MSS-SP-43, ANSI B16.9, ASME B16.28
Specifications: SCH 10 to SCH 160
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 601 uns n06601 elbow fitting in China. If you're going to wholesale high quality inconel alloy 601 uns n06601 elbow fitting made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 601 UNS N06601 elbow fitting introduce
Inconel meatl 601 UNS N06601 elbow fitting


Gnee Steel has a unique portfolio of pipe products designed to create durable pipe components that are a sustainable and premium alternative to help businesses grow. We are manufacturers, suppliers and exporters of Inconel 601 pipe fittings that create effective connections between multiple pipes of various sizes. Our range of Inconel 601 butt weld pipe fittings covers all types of conventional pipe fittings as well as custom fittings that comply with ASTM B366, which covers Inconel 601 pipe fittings in both welded and seamless construction for pressure piping systems and pressure vessel fabrication in medium and high temperature conditions.
Our Inconel 601 butt weld pipe fittings are an indispensable component in the petroleum industry; these pipes feature a one-piece metal body with no porosity, making them a reliable choice for critical transmission housings. In addition, we also offer ASTM B366 UNS NO6601 lap joint stub ends that are reusable, corrosion-resistant, and can be quickly disassembled for inspection. In addition, we also provide a wide range of Inconel 600 ASTM B366 pipe fittings such as Inconel 601 Tees, Inconel 601 End Caps, Inconel 601 Reducers, Inconel 601 Crosses, Inconel 601 Elbows, Inconel 600 Pipe Stubs, etc.
Common Trade Names:
Alloy 601 , Inconel 601 , Nickel 601 , UNS: N06601 , W. Nr: 2.4851 , NS313 , NiCr23Fe
Specifications:
ASTM B163, B166, B167, B168, B564, AMS 5715, 5870, B751, B775, B829
Inconel 601 Chemical Composition
| % | Ni | Cr | Cu | C | Mn | Si | S | Fe | Al |
|---|---|---|---|---|---|---|---|---|---|
| Min | 58 | 21 | - | - | - | - | - | - | 1 |
| Max | 63 | 25 | 1 | 0.1 | 1 | 0.5 | 0.015 | Balance | 1.7 |
Inconel 601 Physical Properties
| Density | Melting range |
|---|---|
| 8.11 g/cm³ | 1360-1411°C |
Inconel 601 Mechanical Properties
| Mechanical & Physical Properties | 21°C | 538°C | 649°C | 760°C | 871°C | 982°C | 1093°C |
|---|---|---|---|---|---|---|---|
| Ultimate Tensile Strength /kMPa | 689.5 | 620.5 | 413.7 | 234.4 | 124.1 | - | - |
| 0.2% Yield Strength /MPa | 372.3 | 331 | 282.7 | 179.2 | 103.4 | - | - |
| Minimum Creep 0.0001% per hr,MPa | - | - | - | 28.3 | 13.8 | 5.2 | 3 |
| 10,000 hr Rupture Strength, MPa | - | - | - | 42.7 | 17.9 | 8.3 | 4.3 |
| Coefficient of Thermal Expansion µm/m⁰C | 15.3 | 16 | 16.6 | 17.1 | 17.6 | 18.3 | |
| Thermal Conductivity /kcal/(hr.m.°C) | 9.7 | 17.3 | 18.9 | 20.4 | 22 | 23.5 | 25.1 |
| Modulus of Elasticity/ 105 MPa | 2.06 | 1.75 | 1.66 | 1.55 | 1.42 | 1.27 | 1.12 |
Inconel 601 Manufacturing And Heat Treatment
Machinability
Alloy 601 can be processed by all conventional processing techniques. The alloy tends to work harden during machining.
Molding
The alloy can be easily formed by all conventional methods. All traces of lubricant must be removed after forming, as the alloy may become brittle at high temperatures.
Welding
Alloy 601 can be welded using traditional welding techniques, such as gas tungsten welding, shielded metal arc welding, and submerged arc welding.
Forging
Forging of 601 alloy can be performed at temperatures ranging from 1038 to 1232°C (1900 to 2250°F).
Hot working
The alloy is hot worked at temperatures from 871 to 1232°C (1600 to 2250°F).
Cold working
The alloy can be cold worked using standard tools.
Standard Specification For ASTM AB366 Inconel 601 Pipe Fittings
Specifications : ASTM B366 / ASME SB366
Dimensions : ASME/ANSI B16.9
Size : 1/8" NB TO 28" NB. (Seamless & 100% X-Ray Welded, Fabricated)
Type : Seamless / Welded / Fabricated
Bending Radius : R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom
Thickness : Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS or Custom Thickness upto 50 MM
GNEE Group Factory Environment
Inconel Alloy UNS N06601 elbow fitting

GNEE Group Product Packaging
601 UNS N06601 elbow fitting


FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: Inconel Alloy 601 UNS N06601 elbow fitting, China Inconel Alloy 601 UNS N06601 elbow fitting suppliers, inconel alloy gear parts, inconel alloy structural parts, inconel alloy fuel system parts, inconel alloy wire harness parts, inconel alloy spinning process, inconel alloy encoder decoder parts
You Might Also Like
Send Inquiry