Inconel Alloy 625 693 Piping
video

Inconel Alloy 625 693 Piping

Available Formats
GNEE Group offers Nickel Alloy Inconel 625 693 in a variety of forms, including:
Bars
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 625 693 piping in China. If you're going to wholesale high quality inconel alloy 625 693 piping made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

inconel Products Application

inconel alloy 625 693 ss piping video

​Inconel 625 Pipe

UNS:

N06625

Specifications:

ASTM B444, ASTM B751, ASTM B829, ASTM B775, ASTM B705, ASTM B704, AMS 5581

International Specifications:

ISO 6207, VdTüV 499, BS 3074NA21, DIN 17751, WERKSTOFF Nr 2.4856

Equivalent material grade of Nickel Alloy 601 pipe

Grade Euronorm Old British GOST UNS No Japanese JIS
AFNOR No En BS
Inconel 601 NC23FeA 2.4851 NiCr23Fe NA 49 XH60BT N06601 NCF 601
inconel Material Specification

Chemical Composition

The chemical composition of INCONEL 693 is outlined in the following table.

Element Content (%)
Nickel. Ni 53.34 - 67.5
Chromium, Cr 27 - 31
Iron, Fe 2.5 - 6
Aluminum, Al 2.5-4
Titanium, Ti ≤ 1
Manganese, Mn ≤ 1
Niobium, Nb 0.50 - 2.5
Copper, Cu ≤ 0.50
Silicon, Si ≤ 0.50
Carbon, C ≤ 0.15
Sulfur, S ≤ 0.010

Inconel 625 (Alloy 625, UNS N06625) Tube/Pipe Specification:

Metal Type: UNS N06625
Tube or pipe: ASTM B444 ASTM B704 AMS 5581 BS3074 GEB50TF133

Chemical Composition, %

  Ni Fe Cr Si Mo Mn C
Max   5.0 23.0 0.50 10.0 0.50 0.10
Min 58.0   20.0   8.0    

inconel alloy 625 693 seamless piping dealeralloy 625 693 piping price

Inconel 625, also known as Alloy 625, is a nickel-chromium-molybdenum alloy with added niobium, which works with the molybdenum to harden the alloy matrix to provide high strength without the need for intensive heat treatment. The alloy is resistant to a variety of severe corrosive environments, especially pitting and crevice corrosion, and has excellent fatigue strength and resistance to chloride ion stress corrosion cracking. Inconel 625 is used in chemical processing, aerospace and marine pipelines, pollution control equipment and nuclear reactors. Typically it can be used at oxidation temperatures up to 980°C [1800°F].
INCONEL 693 alloy (UNS N06693) is a new alloy produced by LAN DONG. It provides high-temperature corrosion resistance that previous nickel-based alloys could not achieve. Of particular interest to designers is the alloy's ability to resist metal dusting. INCONEL 693 alloy provides the best resistance to metal dusting in chemical and petrochemical environments of any alloy currently produced. A typical 693 alloy contains 60.5% nickel, 29% chromium and 3.1% aluminum.

GNEE Group Factory Environment

Inconel Alloy 625 693 Piping

Inconel Alloy 625 693 Piping

Customer Case

customer visit

inconel 625 693 piping dealer

inconel alloy 625 693 stainless piping suppliers

FAQ

 

 

 

Q: How do you make our business establish a long-term and good relationship?
A: We maintain good quality and competitive prices to ensure that our customers benefit; we respect every customer just like our friends and sincerely do business and make friends with them. No matter where they come from.

Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.

Q: About the product price of inconel alloy 625 693 piping?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: inconel alloy 625 693 piping, China inconel alloy 625 693 piping suppliers, Inconel 625 Stainless Steel Coil, inconel alloy metal tube, Inconel Seamless Pipe, inconel alloy amplifier parts, inconel alloy union fittings, inconel alloy transformer parts

Send Inquiry

whatsapp

Phone

E-mail

Inquiry