Inconel Alloy 600 Forgings
Density: 0.304 lb/in3
Melting Range: 2470-2575 degrees Fahrenheit
Specific Heat (Btu/lb F): 0.11
Poisson's Ratio: 0.29
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel alloy 600 forgings in China. If you're going to wholesale high quality inconel alloy 600 forgings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel Alloy 600 Forgings Description

Inconel 600 alloy forgings are components made by shaping a nickel-chromium alloy through various forging processes such as open-die forging or closed-die forging. The alloy is known for its high strength, excellent corrosion resistance, and ability to maintain integrity at high temperatures, making it ideal for demanding applications.
Inconel 600 forgings are relatively unaffected by most neutral and alkaline salt solutions and can even be used in certain alkaline environments. It is resistant to corrosion from steam and mixtures of steam, air, and carbon dioxide. The alloy is nonmagnetic, has excellent mechanical properties, combines high strength with good machinability, and is easily welded. It has cold forming characteristics commonly associated with chromium-nickel stainless steels. It resists oxidizing conditions better than nickel 200 and 201, and due to its high nickel content, also has good resistance to reducing conditions. It exhibits excellent resistance to high-purity water used in nuclear reactors and has good resistance to scaling at high temperatures.
Nickel Alloy 600 Forgings Stock and Supply Range


INCONEL 600 Forging Specifications
| Specifications | ASTM B564, ASME SB564, AMS 5665 |
|---|---|
| Standard | BS 3072-3076 (NA14) DIN 17742, DIN 17750, DIN 17754 WERKSTOFF Nr 2.4816 TÜV 305 AFNOR-NC 15 Fe, DIN, ASTM, BS and all International Standards |
| Flat bar blocks | up to 27″ width and 15,000 lbs |
| Cylinders and sleeves | up to 50″ maximum O.D. and 65″ maximum length |
| Discs and hubs | up to 50″ diameter and 20,000 lbs |
| Rolled, hand forged or mandrel forged rings | up to 84″ maximum O.D. and 40″ maximum length |
| Rounds, shafts and step shafts | up to 144″ maximum length and 20,000 lbs |
| Forging Types | Impression Die Forging, Open Die Forging, Seamless Rolled Forging, Hot Forging, Cold Forging, Open die hammer forging, Impression die drop forging, Closed Die Forging, Press Forging, Upset Forging, Compression Forging, Swaging, Rotary Forging, Roll forging. |
INCONEL 600 FORGINGS EQUIVALENT GRADES
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Inconel 600 | 2.4816 | N06600 | NCF 600 | NA 13 | МНЖМц 28-2,5-1,5 | NC15FE11M | NiCr15Fe |
INCONEL 600 CHEMICAL COMPOSITION FOR FORGINGS
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
MECHANICAL PROPERTIES OF INCONEL 600 FORGINGS
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
About Gnee Steel

Gnee Steel is a professional manufacturer of various nickel-based alloys. Gnee Steel's product packaging includes steel strapping: pipes with an outer diameter of no more than 3 inches are usually strapped together with polypropylene film to prevent rust during sea transportation, and then fixed with steel straps; wooden boxes/crates: pipes are usually packaged in wooden boxes or crates to protect them during transportation, especially pipes with longer lengths or larger diameters; airworthy export packaging: suppliers usually use standard airworthy export packaging methods, which may include various materials and technologies to protect pipes during transportation; rainproof cloth packaging: prevents external rainwater, seawater, etc. from penetrating into the export wooden box packaging during transportation. Gnee Steel specializes in the production and sale of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, nuclear energy and other fields, and can provide customized alloy material solutions according to customer needs. If you need to understand the price of alloy materials or provide customized alloy material solutions, please feel free to contact us for a quote at ss@gneesteel.com
Hot Tags: inconel alloy 600 forgings, China inconel alloy 600 forgings suppliers, Inconel 617 Super Stainless Pipe, inconel alloy integrated circuit parts, inconel tube, inconel alloy plug fittings, inconel alloy transistor parts, inconel alloy valve parts