Inconel 600 Forged Fittings
GNEE Group offers Nickel Alloy Inconel 600 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 forged fittings in China. If you're going to wholesale high quality inconel 600 forged fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Inconel 600 Forged Fittings introduce
Inconel 600 Forged Fittings


Alloy 600 Forged Threaded Fittings has good resistance to oxidation at high temperature. It out performs all other alloys for resistance to nitridation in cracked ammonia. Inconel 718 Forged Threaded Cross should not be used in sulphur containing atmospheres at high temperature, particularly if the conditions are reducing. Inconel 625 Forged Threaded Coupling resists dry chlorine and hydrochloric acid gas at moderate temperatures. Inconel Forged Fittings, Inconel 600 Forged Threaded Union & all other Inconel 625 Forged Pipe Fittings can be hot forged. The surface should be clean before heating. Solution annealing after forging is normal. ASME 16.11 Inconel 601 Socketweld Fittings is readily cold formed by standard processes and equipment. Work hardening in cold forming may require intermediate anneal.
Inconel 600 Forged Fittings to most national and international standards are available, including ASME B16.11 and BS 3799, Inconel 600 Socket Weld and Inconel 600 Screwed Fittings, ASME B16.5, ASME B16.47, BS EN1092 (BS 4504), BS 10, DIN, UNI, NF E 29.
ASTM B564 Inconel Forged Fittings Specification
Specifications : ASTM B564 / ASTM SB 564
Type : Socketweld Fittings, Screwed-Threaded Fittings
Size : ⅛" to 4"
Class :2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Standards : ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Inconel 600 Forged Fittings Equivalent Grade
| STANDARD | WERKSTOFF NR. | UNS | AFNOR | GOST | JIS | BS | EN | OR |
| Inconel 600 | 2.4816 | N06600 | NC15FE11M | МНЖМц 28-2,5-1,5 | NCF 600 | NA 13 | NiCr15Fe | ЭИ868 |
Inconel 600 Socketweld Forged Fittings Chemical Composition
| Grade | Cr | Fe | Ni | C | Mn | Cu | Si | S |
| Inconel 600 | 14.0 – 17.0 | 6.0 – 10.0 | 72.0 min | 0.15 max | 1.0 max | 0.5 max | 0.5 max | 0.015 max |
Alloy 600 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
GNEE Group Factory Environment
Inconel 600 Forged Fittings

FAQ
Q:Can we visit your factory ?
A:Warmly welcome once we have your schedule we will pick you up .
Q: Do you have quality control?
A: Yes, we have gained BV, SGS authentication.
Q: Can you arrange the shipment?
A: Sure, we have permanent freight forwarder who can gain the best price from most ship company and offer professional service.
Hot Tags: inconel 600 forged fittings, China inconel 600 forged fittings suppliers, inconel alloy resin transfer molding process, inconel alloy reaction injection molding process, Inconel UNS N07718 Pipe Fitting, inconel alloy switch parts, inconel alloy valve parts, inconel alloy spindle parts
You Might Also Like
Send Inquiry