Thick wall Inconel 718SPF polished pipe
GNEE Group offers Nickel Alloy Inconel 718 in a variety of forms, including:
Bars
Wires
Sheets
Forgings
Tubes
Flanges
Seamless and Welded Pipes
Welding Rods
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of thick wall inconel 718spf polished pipe in China. If you're going to wholesale high quality thick wall inconel 718spf polished pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Thick wall Inconel 718SPF polished pipe introduce
INCONEL alloy 718SPF is a specifically "tailored" version of INCONEL alloy 718, designed for the superplastic forming process. The alloy is optimized for the process by rigorous control of composition, melt practice and rolling conditions.
Thick wall Inconel 718SPF pipe


Overview
As a leading supplier & manufacturer in China, GNEE group supply cost-effective Inconel 718SPF Products.
INCONEL alloy 718SPF is a specifically "tailored" version of INCONEL alloy 718, designed for the superplastic forming process. The alloy is optimized for the process by rigorous control of composition, melt practice and rolling conditions.
INCONEL alloy 718SPF was developed to meet the need for a nickel-base alloy suitable for manufacture into complex shaped components subject to a combination of high temperature, high temperature corrosion and high stress. INCONEL alloy 718SPF meets all the mechanical property requirements of AMS 5596G, as annealed plus aged, as well as all requirements of AMS 5950, which is specific to INCONEL alloy 718SPF.
Superplastic forming, now highly sophisticated and used extensively for producing commercial and military aircraft components, is an ideal process for manufacturing complex shaped parts. Use of superplastic forming can enhance component performance and reliability while lowering overall manufacturing cost by reducing the need for extensive welding or other joining methods, lowering the inventory of parts and simplifying the manufacturing process.
Mechanical Properties
INCONEL alloy 718SPF is produced with an annealed temper. The alloy is produced to a grain size of ASTM No. 10 (0.01 mm/0.0004 in) or finer. As produced, INCONEL alloy 718SPF sheet meets the strength and ductility requirements of AMS 5596G, as annealed plus aged.
Corrosion Resistance
INCONEL alloy 718SPF, like alloy 718, has excellent resistance to corrosion in many media. This characteristic, similar to that of other nickel-chromium alloys, is a function of its composition.
Nickel contributes to a resistance to corrosion by many inorganic and organic compounds, other than those that are strongly oxidizing, throughout wide ranges of acidity and alkalinity. It is also useful in providing resistance to chloride- ion stress-corrosion cracking. Chromium imparts an ability to withstand attack by oxidizing media and sulfur compounds. Molybdenum is know to contribute to resistance to pitting in many media.
Above all, INCONEL alloy 718SPF is important for its strength and corrosion resistance at high operating temperatures.
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 8.22 | |
|---|---|---|---|
| lb/in.3 | 0.297 | ||
| Melting Range | °F | 2300 - 2437 | |
| °C | 1260 - 1335 | ||
| Specific Heat | Btu/lb-°F | 0.104 | |
| J/kg-°C | 435 | ||
| Curie Temperature | °F | -170 | |
| °C | -113 | ||
| Permeability at 200 oersted | 15.9 kA/m | 1.0011 | |
Mechanical Properties
| INCONEL alloy 718SPF Annealed |
AMS 5596G Solution Annealed |
AMS 5950 Solution Annealed |
|
|---|---|---|---|
| Room Temperature Tensile Properties | |||
| 0.2% Y.S., ksi (MPa) | 120 (829) | 80 (552) max. | 155 (1069) max. |
| U.T.S., ksi (MPa) | 162 (1117) | 140 (965) max. | 185 (1276) max. |
| Elongation, % | 31 | 30 min. | 20 min. |
| Hardness, Rc | 24 | 25.5 max. | 34 max. |
| Grain Size, ASTM No. | 12 | - | 10 or finer |
| Aged | |||
| 0.2% Y.S., ksi (MPa) | 202 (1393) | 150 (1034) min. | 148 (1020) min. |
| U.T.S., ksi (MPa) | 225 (1551) | 180 (1241) min. | 180 (1241) min. |
| Elongation, % | 16 | 12 min. | 12 min. |
| Hardness, Rc | 45 | 36 min. | 36 min. |
| 1200°F (649°C) Tensile Properties | Aged | ||
| 0.2% Y.S., ksi (MPa) | 160 (1103) | 120 (827) min. | 120 (827) min. |
| U.T.S., ksi (MPa) | 177 (1220) | 145 (1000) min. | 145 (1000) min. |
| Elongation, % | 22 | 5 min. | 5 min. |
| 1200°F (649°C) /100 ksi (690 MPa) Stress Rupture Properties | Aged | ||
| Life, h | 95 | 23.0 min. | 23.0 min. |
| Elongation, % | 11.2 | 4 min. | 4 min. |
GNEE Group Factory Environment

GNEE Group Product Packaging
GNEE Group 718SPF polished pipe Packaging

FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: Thick wall Inconel 718SPF polished pipe, China Thick wall Inconel 718SPF polished pipe suppliers, inconel alloy camshaft parts, inconel alloy switch parts, inconel alloy multiplexer parts, inconel tube, inconel alloy thermoforming process, alloy inconel piping
Previous
Inconel 725You Might Also Like
Send Inquiry